采用静电纺丝法以三氟乙酸(TFA)为溶剂制备再生桑蚕丝素(RSF)/醋酸纤维素(CA)共混纳米纤维.通过扫描电镜(SEM),X射线衍射(XRD),X射线光电子能谱(XPS)分别研究不同CA添加量SF/CA共混纤维毡的微观形貌,晶体结构及表面化学性质.结果表明:SF中CA添加量小于10%,共混体系静电纺得到的纤维宏观上呈现均一形貌,但纤维直径变粗;当CA添加量大于20%时,SF与CA两者分相,所得纤维的直径分布加宽,并出现两极分化现象.XPS测试结果显示SF/CA共混纳米纤维中CA的"C"元素的特征峰消失,287.8eV和285.0eV处C1s的峰转化为285.0eV处的窄峰.共混后纤维力学性能明显改善.

参考文献

[1] Cham Vepari;David L.Kaplan .Silk as a biomaterial[J].Progress in Polymer Science,2007(8/9):991-1007.
[2] Gunaranjan Viswanathan;Saravanababu Murugesan;Victor Pushparaj;Omkaram Nalamasu;Pulickel M.Ajayan .Preparation of Biopolymer Fibers by Electrospinning from Room Temperature Ionic Liquids[J].Biomacromolecules,2006(2):415-418.
[3] A potential material for tissue engineering: Silkworm silk/PLA biocomposite[J].Composites, Part B. Engineering,2008(6):p.1026-1033.
[4] Zhang, F;Zuo, BQ;Zhang, HX;Bai, L .Studies of electrospun regenerated SF/TSF nanofibers[J].Polymer,2009(1):279-285.
[5] 赵瑾,赵玉平,张伟,袁晓燕.PLGA/明胶共混体系的静电纺丝研究[J].高等学校化学学报,2009(02):391-395.
[6] Jianxin He;Yuyuan Tang;Shan-Yuan Wang .Differences in Morphological Characteristics of Bamboo Fibres and other Natural Cellulose Fibres: Studies on X-ray Diffraction, Solid State ~(13)C-CP/MAS NMR, and Second Derivative FTIR Spectroscopy Data[J].Iranian polymer journal,2007(12):807-818.
[7] Won Ho Park;Lim Jeong;Dong Ii Yoo;Sam Hudson .Effect of chitosan on morphology and conformation of electrospun silk fibroin nanofibers[J].Polymer: The International Journal for the Science and Technology of Polymers,2004(21):7151-7157.
[8] 薛华育,顾卓,戴礼兴,白伦.再生丝素/聚乙烯醇共混纳米纤维的制备及表征[J].高分子材料科学与工程,2007(06):240-243.
[9] Desai, K;Kit, K;Li, JJ;Davidson, PM;Zivanovic, S;Meyer, H .Nanofibrous chitosan non-wovens for filtration applications[J].Polymer: The International Journal for the Science and Technology of Polymers,2009(15):3661-3669.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%