通过拉伸实验研究电化学充氢对5Cr油管钢拉伸性能的影响表明:随充氢时间和充氢电流密度的增加,5Cr油管的强度和塑性有所减小.用扫描电镜(SEM)观察断口发现其形貌以韧窝为主要特征,与未充氢试件相比,充氢试样拉伸断裂后韧窝尺寸变小、变浅,数量增多,这说明材料的塑性损失增大.充氢到一定值后材料由韧性断裂转变为脆性断裂.

Tensile tests were used to investigate the mechanical behaviors of 5Cr tubing after electrochemical hydrogen charging. The experiment results show that the tensile strength and the plasticity decreased with the increase of pre-charging time and pre-charging density. Analysis on the fracture morphology by scanning electron microscope (SEM) indicated that the fracture surfaces of 5Cr tubing were characteristic of ductile dimple fracture pattern after electrochemical hydrogen charging. The diameter and depth of ductile dimple were smaller than the specimen without charging, but the number of ductile dimple was increased, which means that the loss of plastic properties was increased. When the hydrogen concentration reached a certain value, the fracture mode was changed from ductile fracture to brittle fracture.

参考文献

[1] D.Delafosse;T.Magnin .Hydrogen induced plasticity in stress corrosion cracking of engineering systems[J].Engineering Fracture Mechanics,2001(6):693-729.
[2] 赵颖,王荣.X70管线钢电化学充氢后的力学行为研究[J].中国腐蚀与防护学报,2004(05):293-296.
[3] 张士欢,王荣.X80管线钢电化学充氢后的断裂特性研究[J].石油机械,2008(01):16-18.
[4] 张颖瑞,董超芳,李晓刚,芮晓龙,周和荣.电化学充氢条件下X70管线钢及其焊缝的氢致开裂行为[J].金属学报,2006(05):521-527.
[5] 张涛,龙军,孙新岭,陈居术.管道钢X80氢渗透实验研究[J].后勤工程学院学报,2003(01):16-18.
[6] 张涛,李著信,苏毅,陈居术,林梅.X80管线钢氢致断裂断口分析[J].机械工程材料,2004(03):13-15.
[7] 王荣.氢对X70管线钢预裂纹试样断裂性能的影响[J].中国腐蚀与防护学报,2008(02):81-85.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%