The spinel compound Li(4)Ti(5)O(12) was synthesized by a solid state method. In this synthesizing process, anatase TiO(2) and Li(2)CO(3) were used as reactants. The influences of reaction temperature and calcination time on the properties of products were studied. When calcination temperature was 750 degrees C and calcination temperature was 24 h, the products exhibited good electrochemical properties. Its discharge capacity reached 160mAh g(-1) and its capacity retention was 97% at the 50th cycle when the current rate was 1 C. When current rate increased to 10 C, its first discharge capacity could reach 136mAh g(-1), and its capacity retention was 85% at the 50th cycle. (C) 2011 Elsevier B.V. All rights reserved.