回顾并评述了目前世界范围内的主流的“未爆先漏(LBB)”理论,指出LBB评定图技术是目前较能适合工程安全评定并被广泛应用的LBB准则.综述了LBB技术应用现状,指出LBB技术在压力容器设计方面的应用还仅处于初级的理想状态;而LBB技术在压力容器评定方面的应用,先漏后爆(LBB)评定图的改造、裂纹扩展稳定性分析及泄漏率的计算是亟待解决的问题,为下一步LBB技术应用研究工作指明了方向.
参考文献
[1] | 郑敏荣.先漏后爆准则的研究[J].北京石油化工学院学报,2003(02):28-32. |
[2] | Zdarek J.;Kadecka P.;Pecinka L. .LEAK-BEFORE-BREAK CRITERION APPLIED TO VVER 440/230 UNIT[J].Theoretical and Applied Fracture Mechanics,1995(2):117-123. |
[3] | Bergman M;Brickstad B .A procedure for analysis of leak before break in pipes subjected to fatigue or IGSCC accounting for complex crack shapes[J].Fatigue & Fracture of Engineering Material & Structure,1995,18(10):1173-1188. |
[4] | Arzhaev A I;Bougaenko S E;Denisov I N et al.Leakbefore-break criteria and strength monitoring implementation impact on in-service inspection of RBMKprimary circuit components[J].International Journal of Pressure Vessels and Piping,1996,66:359-365. |
[5] | Bartholome G.;Wellein R. .LEAK-BEFORE-BREAK BEHAVIOR OF NUCLEAR PIPING SYSTEMS[J].Theoretical and Applied Fracture Mechanics,1995(2):145-149. |
[6] | Bartholomé G;Faidy C;Franco C .Application of leakbefore-break concept in VVER 440-230 Results and consequences for TACIS-program[J].Nuclear Engineering and Design,1997,176:285-295. |
[7] | Chung D Y;Lim H S.Applicability of LBB (Leak-before-break) design for main steam line in Korea nuclear power plant[A].Washington DC(US),2001:1-7. |
[8] | Irwin G R.Materials for missiles and spacecraft[J].Pressure Vessel Fracture,1963:204-229. |
[9] | J E Hood .Fracture of steel pipelines[J].International Journal of Pressure Vessels and Piping,1974,2(03):165-178. |
[10] | Vijay G;Ukadgaonker R;Shanmuga B .Review of work related to ' leak-before-break ' assessment[J].International Journal of Pressure Vessels and Piping,1996,69(02):135-148. |
[11] | 周道祥,刘安中.压力容器"破前漏"准则的实验研究[J].压力容器,2003(04):10-13. |
[12] | Sharples J K;Clayton A M .A leak-before-break assessment method for pressure vessels and some current unresolved issues[J].International Journal of Pressure Vessels and Piping,1990,43(1-3):317-327. |
[13] | Sturm D;Stoppler W .Strength behavior of flawed pipes under internal pressure and external bending moment:Comparison between experiment and calculation[J].International Journal of Pressure Vessels and Piping,1990,43(1-3):351-366. |
[14] | 吴清可.防脆断设计[M].北京:机械工业出版社,1991 |
[15] | BS 7910:2005.Guide to methods for assessing the acceptability of flaw in metallic structures[S].Standards Policy and Strategy Committee,2005. |
[16] | Structure integrity assessment procedure for European industry project BE 95-1426[S].Final Procedure,British Steel Report |
[17] | IAEA-TECDOC-710.Applicability of the leak before break concept[S].International Atomic Energy Agency,1993. |
[18] | Wichman K;Lee S .Development of USNRC standard review plan 3.6.3 for leak-before-break applications to nuclear power plants[J].International Journal of Pressure Vessels and Piping,1990,43(1-3):57-65. |
[19] | 郑炜,董亚民,孙学伟.LBB稳定性研究的可靠性分析及临界裂纹长度计算[J].工程力学,2004(01):72-76. |
[20] | Zahoor A.Ductile Fracture Handbook[M].RP 1757-69,Novetech Corporation and EPRI,1990 |
[21] | 董亚民,冯峰,黄克智.压力容器及管道LBB稳定性分析的工程估算方法[J].工程力学,2000(01):13. |
[22] | 冯西桥;何树延 .表面裂纹疲劳扩展的一种损伤力学方法[J].清华大学学报(自然科学版),1997,37(05):78-82. |
[23] | 冯西桥;何树延 .管道中表面裂纹的疲劳扩展研究[J].清华大学学报(自然科学版),1998,38(07):35-38. |
[24] | Chivers T C;Mitchell L A .On the limiting velocity through parallel bore tubes[J].Journal of Physics D:Application Physics,1971,4:1069-1076. |