The 304 stainless steel (SS) microcantilever specimens with dimensions of 30 μm×30 μm×50μm (thickness×width × length) were fabricated by femtosecond (fs) laser. The microsized cantilevers of good quality with structure and dimensions according commendably with that of the designed cantilever were obtained. The result shows that fs laser micromachining is a promising method for directly fabricating metallic microcomponents.Corrosion and fatigue properties of microsized specimens were carried out on the microsized 304 SS cantilever beams by a newly developed fatigue testing machine. The results show that the microsized 304 SS specimens appear to have an improved resistance towards localized corrosion compared to ordinary-sized 304 SS specimens after the static corrosion testing. The testing result shows that the presence of corrosive solution reduces the fatigue lifetime of the 304 SS specimen by a factor of 10-100. The maximum bending loads measured by fatigue testing machine decrease rapidly at the terminal stage of environment assisted fatigue testing.Corrosion fracture first occurred at the range of notch with a higher tensile bending stress, and exhibited clear evidence of trans-columnar fracture detected by SEM (scanning electron microscopy).

参考文献

[1] W.H.Chuang;K.F.Rainer;G.Reza .[J].Sensors and Actuators A:Physical,2005,121(15):557.
[2] X.D.Li;B.Bharat .[J].Surface & Coatings Technology,2003,163-164(521):521.
[3] C.W.Baek;Y.K.Kim;Y.Ahn;Y.H.Kim .[J].Sensors and Actuators A:Physical,2005,117(19):17.
[4] S.Sriram;B.Bharat .[J].Sensors and Actuators A:Physical,2002,101(21-22):338.
[5] G.P.Zhang;K.Takashima;M.Shimojo;Y.Higo .[J].Materials Letters,2003,57:1555.
[6] A.P.Jivkov .[J].Theor Avpl Fract Mec,2003,40(26):45.
[7] C.L.Muhlstein;S.B.Brown;R.O.Ritchie .[J].Journal of Microelectromechanical Systems,2001,11(07):593.
[8] C. L. Muhlstein;E. A. Stach;R. O. Ritchie .Mechanism of fatigue in micron-scale films of polycrystalline silicon for microelectromechanical systems[J].Applied physics letters,2002(9):1532-1534.
[9] N.V.Lavrik;M.J.Sepaniak;P.G.Datskos .[J].Review of Scientific Instruments,2004,75(08):2229.
[10] R.Berger;C.Gerber;J.K.Gimzewski;E.Meyer and H.J.Guntherodt .[J].Applied Physics Letters,1996,69(07):40.
[11] S.M.Spearing .Matrials issues in micrelectromechanical systems (MEMS)[J].Acta materialia,2000(1):179-196.
[12] K.Takashima;Y.Higo;S.Sugiura;M.Shimojo .[J].Materials Transactions,2001,42(03):68.
[13] M.Diener;C.Kowanda .[J].Materials and Manufacturing Processes,2004,19(01):111.
[14] J.Peirs;D.Reynaerts;F.Verplaetsen .[J].Sensors and Actuators A:Physical,2004,113(10):86.
[15] X.Liu;D.Du;G.Mourou .[J].IEEE Journal of Quantum Electronics,1997,33(20):1706.
[16] A.Borowiec;H.K.Haugen .Femtosecond laser micromachining of grooves in indium phosphide[J].Applied physics, A. Materials science & processing,2004(3):521-529.
[17] H.Dachraoui;W.Husinsky .[J].Applied Physics Letters,2006,89(08):104102.
[18] X.D.Li;B.Bhushan .[J].Scripta Materialia,2002,47(03):473.
[19] J. W. Schultze;V. Tsakova .Electrochemical microsystem technologies: from fundamental research to technical systems[J].Electrochimica Acta,1999(21/22):3605-3627.
[20] J.W.Schultze;A.Bressel .[J].Electrochimica Acta,2001,47(01):3.
[21] J.Heinze .[J].Angewandte Chemie International Edition,1993,32(02):1268.
[22] J.H.Xie;A.T.Alpas;D.Northwood .[J].Materials Characterization,2002,48(02):271.
[23] K. Tokaji;H.-N. Ko;M. Nakajima .Effects of humidity on crack initiation mechanism and associated S-N characteristics in very high strength steels[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2003(1/2):197-206.
[24] G.P.Zhang;K.Takashima;Y.Higo .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2006,426(03):96.
[25] X.Li;B.Bhushan .[J].Materials Characterization,2002,48:11.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%