当Ti-6Al-4V合金层厚度达到0.7 mm时(板材总厚2 mm),室温强度和延伸率分别超过800 MPa和4%,700 ℃条件下延伸率超过25%.

参考文献

[1] Edward A. Loria .Gamma titanium aluminides as prospective structural materials[J].Intermetallics,2000(9/11):1339-1345.
[2] 孔凡涛,陈子勇,田竞,陈玉勇.提高TiAl基合金室温塑性的方法[J].稀有金属材料与工程,2003(02):81-86.
[3] CHEN Yu-yong;KONG Fan-tao;TIAN Jing .Recent developments in engineering gamma-TiAl intermetallics[J].Transactions of Nonferrous Metals Society of China,2002(4):605-609.
[4] Ramanujan R V .[J].International Materials Reviews,2000,45(06):217.
[5] Arno Bartels;Heinrich Kestler;Helmut Clemens .[J].Materials Science and Engineering,2002,A329/331:153.
[6] Yu T H;Koo C H .[J].Scripta Materialia,1998,39(07):915.
[7] Koeppe C;Bartels A;Clemens H et al.[J].Materials Science and Engineering,1995,A201:182.
[8] Inkson B J;Clemens H;Marien J .[J].Scripta Materialia,1998,38(09):1377.