采用高温固相反应法制备尖晶石相Li4Ti5O12负极材料.初步研究了反应温度和反应时间对Li4Ti5O12电化学性能的影响.XRD衍射未观测到TiO2残余存在;电化学测试显示,1.2~2.5V恒流充放电,其可逆容量达158.3mAh/g,首次库仑效率为95.2%;循环20周其容量衰减率仅为3.1%.
参考文献
[1] | Tarascon J M;Armand M .[J].Nature,2001,414:359-367. |
[2] | Hasegawa K;Arakawa Y .[J].Journal of Power Sources,1993,43-44:523-529. |
[3] | Dahn J R;Fuller E W;Obrovac M et al.[J].Solid State Ionics,1994,69:265-270. |
[4] | Croce F;Appetecchi G B;Persi L et al.[J].Nature,1998,394:456-458. |
[5] | Thackeray M M .[J].Progress in Solid State Chemistry,1997,25:1-71. |
[6] | Ronci F;Stallworth P E et al.[J].Journal of Power Sources,2003,119-121:631-636. |
[7] | Ariyoshi K;Yamato R;Ohzuku T .[J].Electrochimica Acta,2005,51:1125-1129. |
[8] | Guerfi A;Sevigny S et al.[J].Journal of Power Sources,2003,119-121:88-94. |
[9] | Jansen A N;Kahaian A J et al.[J].Journal of Power Sources,1999,81-82:902-905. |
[10] | Wen Zhaoyin;Gu Zhonghua et al.[J].Journal of Power Sources,2005,146:670-673. |
[11] | 苏岳锋,吴锋,陈朝峰.纳米微晶TiO2合成Li4Ti5O12及其嵌锂行为[J].物理化学学报,2004(07):707-711. |
[12] | Ohzuku T.;Yamamoto N.;Ueda A. .ZERO-STRAIN INSERTION MATERIAL OF LI[LI1/3TI5/3]O-4 FOR RECHARGEABLE LITHIUM CELLS[J].Journal of the Electrochemical Society,1995(5):1431-1435. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%