利用纤维Z-pins的细观力学模型构造了相应的Z-pin单元,结合考虑一阶剪切变形的梁单元,建立了用于分析含非对称分层采用Z-pins增韧的端部开口弯曲试件(End notched flexure,ENF)的有限元模型,并在分层裂纹面上引入接触单元以防止分析过程中2个分层子梁在端部开口处的相互嵌入.通过数值算例分析了Z-pins对含非对称分层的ENF试件Ⅱ型层间韧性的增强作用.参数分析表明,当分层位置靠近层合板的表面时,Z-pins的增韧作用明显下降,Z-pins对Ⅱ型层间韧性的增强作用主要由2个分层子层中较薄子层决定,但另一分层的厚度也对Ⅱ型层间韧性有一定的影响.

参考文献

[1] Abrate S.Impact on laminated composites:Recent advances[J].Applied Mechanics Review,1994,47(11):517-544.
[2] 沈真.复合材料损伤与断裂的研究进展[C]//复合材料及其结构力学进展.范赋群主编.武汉:武汉工业大学出版社,1992.Shen Zhen.Advances on damage and fracture of composite materials[C]// Advances on Composite Materials and Structures.Fan Fuqun ed.Wuhan:Press of Wuhan Industrial University,1992.
[3] 孙先念,郑长良.层合复合材料Z-pinning增强技术的力学进展[J].航空学报,2006,27(6):1194-1202.Sun Xiannian,Zheng Changliang.Advances on modeling through-the-thickness reinforcement of laminated composite by Z-pinning[J].Acta Aeronautiea et Astronautica Sinica,2006,27(6):1194-1202.
[4] Freitas G,Magee C,Dardzinski P,Fusco T.Fiber insertion process for improved damage tolerance in aircraft laminates[J],Journal of Advanced Materials,1994,25(4):36-43.
[5] Partridge I K,Carrie D D R.Delamination resistant laminates by Z-fiber pinning Ⅰ:Manufacture and fracture performance[J].Composites Part A,2005,36(1):55-64.
[6] Jain L K,Dransfield K A,Mai Y W.On the effect of stitching in CFRPs--Ⅱ:Mode Ⅱ delamination toughness[J].Composites Science and Technology,1998,58(6):829-837.
[7] Yan W,Liu H Y,Mai Y W.Numerical study on the mode Ⅰdelamination toughness of Z-pinned laminates[J].Composites Science and Technology,2003,63(10):1481-1493.
[8] Grassi M,Zhang X.Finite element analyses of mode Ⅰinterlaminar delamination in Z-fibre reinforced composite laminates[J].Composites Science and Technology,2003,63(12):1815-1832.
[9] Cox B N.Constitutive model for a fiber tow bridging a delamination crack[J].Mechanics of Composite Materials and Structures,1999,6:117-138.
[10] Cox B N,Sridhar N.A traction law for inclined fibre tows bridging mixed mode cracks[J].Mechanics of Advanced Materials and Structures,2002,9:229-331.
[11] 韩立军,李铁虎,刘建军,邱海鹏,丁海英.采用Z-pin增强体的3D炭/炭复合材料层间断裂行为[J].新型炭材料,2004,19(Z):97-102.Han Lijun,Li Tiehu.Liu Jianjun,Qiu Haipeng,Ding Haiying.Delamination fracture behavior of 3D carbon/carbon composites reinforced by Z-pins[J].New Carbon Materials,2004,19(2):97-102.
[12] Tong L,Sun X.Bending effect of through-thickness reinforcement rods on mode Ⅰ delamination toughness of DCB specimen Ⅰ:Linearly elastic and rigid-perfectly plastic analysis[J].International Journal of Solids and Structures,2004,41(24/25):6831-6852.
[13] Tong Liyong,Sun Xiannian.Bending effect of throughthickness reinforcement rods on mode Ⅱ delamination toughness of ENF specimen:Elastic and rigid-perfectly plastic analyses[J].Composites Part A:Applied Science and Manufacturing,2007,38(2):326-336.
[14] Michael D K W,Sun Xiannian,Tong Liyong,Anthony K,Luo Quantian,Adrian R.A new ENF test specimen for the mode Ⅱ delamination toughness testing of stitched woven CFRP laminates[J].Journal of Composite Materials,2007,41(14):1743-1772.
[15] Rybicki E F,Kanninen M F.A finite element calculation of stress intensity factors by modified crack closure integral[J].Engineering Fracture Mechanics,1977,9:931-938.
[16] Hutchinson J W,Suo Z.Mixed mode cracking in layered materials[J].Advanced Applied Mechanics,1991,29:63-191.