为了保护海洋生态环境,将可生物降解的聚合物材料用于海洋防污涂料,已成为海洋防污涂料的发展方向.介绍了影响聚合物降解性能的主要因素,如化学键类型、使用环境pH值、共聚物组分含量、分子结构等,综述了聚氨酯类、聚酯类、聚酸酐类等生物降解型海洋防污涂料的研究现状,指出了存在的问题和未来的发展方向.
参考文献
[1] | Michael A. Champ .Economic and environmental impacts on ports and harbors from the convention to ban harmful marine anti-fouling systems[J].Marine pollution bulletin,2003(8):935-940. |
[2] | Hideto Tsuji;Kensaku Ikarashi .In vitro hydrolysis of poly(L-lactide) crystalline residues as extended-chain crystallites Ⅲ. Effects of pH and enzyme[J].Polymer Degradation and Stability,2004(1):647-656. |
[3] | Rupei Tang;R. Noelle Palumbo;Weihang Ji .Poly(ortho ester amides): Acid-Labile Temperature-Responsive Copolymers for Potential Biomedical Applications[J].Biomacromolecules,2009(4):722-727. |
[4] | Tang, R.;Ji, W.;Panus, D.;Palumbo, R.N.;Wang, C. .Block copolymer micelles with acid-labile ortho ester side-chains: Synthesis, characterization, and enhanced drug delivery to human glioma cells[J].Journal of Controlled Release: Official Journal of the Controlled Release Society,2011(1):18-27. |
[5] | Zhao ZX;Yang L;Hu YF;He Y;Wei J;Li SM .Enzymatic degradation of block copolymers obtained by sequential ring opening polymerization of L-lactide and epsilon-caprolactone[J].Polymer Degradation and Stability,2007(10):1769-1777. |
[6] | Harro Antheunis;Jan-Cees van der Meer;Matthijs de Geus .Autocatalytic Equation Describing the Change in Molecular Weight during Hydrolytic Degradation of Aliphatic Polyesters[J].Biomacromolecules,2010(4):1118-1124. |
[7] | Liu, F;Zhao, ZX;Yang, J;Wei, J;Li, SM .Enzyme-catalyzed degradation of poly(L-lactide)/poly(epsilon-caprolactone) diblock, triblock and four-armed copolymers[J].Polymer Degradation and Stability,2009(2):227-233. |
[8] | Ma, CF;Hou, Y;Liu, S;Zhang, GZ .Effect of Microphase Separation on the Protein Resistance of a Polymeric Surface[J].Langmuir: The ACS Journal of Surfaces and Colloids,2009(16):9467-9472. |
[9] | Chunfeng Ma;Liguo Xu;Wentao Xu .Degradable polyurethane for marine anti-biofouling[J].Journal of Materials Chemistry, B. materials for biology and medicine,2013(24):3099-3106. |
[10] | 何庆光,王晶晶,叶章基,任润桃.防污涂料用可降解聚氨酯树脂基料的合成研究[J].材料开发与应用,2009(06):19-23,32. |
[11] | Rajan B. Bodkhe;Stephanie E. M. Thompson;Carolyn Yehle .The effect of formulation variables on fouling-release performance of stratified siloxane-polyurethane coatings[J].Journal of coatings technology and research,2012(3):235-249. |
[12] | WangJJ;LiuC;HuangCS et al.Research in the Degradation and Antifouling Performance of Copolyesters of L-Lactide and ε-Caprolactonen[J].Corrosion & Protection,2012,33(Sup2):49-54. |
[13] | Fay F;Linossier I;Langlois V et al.Degradation and Controlled Release Behavior of ε-Caprolactone Copolymers in Biodegradable Antifouling Coatings[J].Biomacromolecules,2006,7(03):851-857. |
[14] | Fay F;Renard E;Langlois V;Linossier I;Vallee-Rehel K .Development of poly(epsilon-caprolactone-co-L-lactide) and poly(epsilon-caprolactone-co-delta-valerolactone) as new degradable binder used for antifouling paint[J].European Polymer Journal,2007(11):4800-4813. |
[15] | Ishimaru, N.;Tsukegi, T.;Wakisaka, M.;Shirai, Y.;Nishida, H. .Effects of poly(L-lactic acid) hydrolysis on attachment of barnacle cypris larvae[J].Polymer Degradation and Stability,2012(11):2170-2176. |
[16] | Fabienne Fa;Isabelle Linossier;Gaelle Legendre;Karine Vallée-Réhel .Micro-Encapsulation and Antifouling Coatings: Development of Poly(lactic acid) Microspheres Containing Bioactive Molecules[J].Macromolecular symposia,2008(0):45-51. |
[17] | Langlois V;Vallee-Rehel K;Peron J J et al.Synthesis and hydrolytic degradation of graft copolymers containing poly (lactic acid) side chains:in vitro release studies of bioactive molecules[J].Polymer Degradation and Stability,2002,76(03):411-417. |
[18] | Ishimoto K;Arimoto M;Ohara H et al.Biobased Polymer System:Miniemulsion of Poly(alkylmethacrylate-graft-lactic acid) s[J].Biomacromolecules,2009(10):2719-2723. |
[19] | Kiyoaki Ishimoto;Maho Arimoto;Tomoya Okuda .Biobased Polymers: Synthesis of Graft Copolymers and Comb Polymers Using Lactic Acid Macromonomer and Properties of the Product Polymers[J].Biomacromolecules,2012(11):3757-3768. |
[20] | Okuda, T.;Ishimoto, K.;Ohara, H.;Kobayashi, S. .Renewable biobased polymeric materials: Facile synthesis of itaconic anhydride-based copolymers with poly(l -lactic acid) grafts[J].Macromolecules,2012(10):4166-4174. |
[21] | Fay F;Linossier I;Langlois V;Vallee-Rehel K;Krasko MY;Domb AJ .Protecting biodegradable coatings releasing antimicrobial agents[J].Journal of Applied Polymer Science,2007(6):3768-3777. |
[22] | Fabienne Fay;Isabelle Linossier;Valerie Langlois .Biodegradable Poly(ester-anhydride) for New Antifouling Coating[J].Biomacromolecules,2007(5):1751-1758. |
[23] | Ma, C.;Yang, H.;Zhou, X.;Wu, B.;Zhang, G..Polymeric material for anti-biofouling[J].Colloids and Surfaces, B. Biointerfaces,2012:31-35. |
[24] | Chun-feng Ma,Hong-jun Yang,Guang-zhao Zhang.ANTI-BIOFOULING BY DEGRADATION OF POLYMERS[J].高分子科学(英文版),2012(03):337-342. |
[25] | Roland Hany;Christine Bohlen;thomas Geiger;Manfred Schmid;Manfred Zinn .Toward Non-Toxic Antifouling:Synthesis of Hydroxy-,Cinnamic Acid-,Sulfate-,and Zosteric Acid-Labeled Poly[3-hydroxyalkanoates][J].Biomacromolecules,2004(4):1452-1456. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%