用ESCA, XRD, SEM及TPR等手段表征了不同条件下再生的工业失活加氢裂化催化剂. 结果表明, Mo-Ni/USY-Al2O3失活催化剂在实验室装置中快速再生优于慢速再生; 再生温度对催化剂的结构与性能有影响. 480 ℃再生能将失活催化剂中绝大部分的碳和氮烧掉,且比表面积恢复率最高; 600 ℃再生时,催化剂的毛细孔口明显减少,且产生少量聚结态β-NiMoO4晶相.

参考文献

[1] Shiring F J;Venkatadri R;Goodwin J G Jr .[J].Canadian Journal of Chemical Engineering,1983,61(02):218.
[2] Bonardet J L;Barrage M C;Fraissard J et al.[J].Studies in Surface Science and Catalysis,1994,88:265.
[3] Guisnet M;Magnoux P .[J].Studies in Surface Science and Catalysis,1994,88:53.
[4] Menon P G .[J].Journal of Molecular Catalysis,1990,59(02):207.
[5] 刘伟;李志林;赵修林 .[J].石油学报(石油加工),1995,11(03):36.
[6] Wiwel P;Zeuthen P;Jacobsen A C.Catalyst Deactivation[M].Amsterdam: Elsevier,1991:257.
[7] Magnoux P;Cartraud P;Mignard S et al.[J].Journal of Catalysis,1987,106(01):235.
[8] Zeuthen P;Bartholdy J;Wiwel P et al.[J].Studies in Surface Science and Catalysis,1994,88:199.
[9] Marinkovic-Neduin R;Bokovic G;Ki E et al.[J].Applied Catalysis A:General,1994,107:133.
[10] 王宗贤,郭爱军,阙国和.辽河渣油热转化和加氢裂化过程中生焦行为的研究[J].燃料化学学报,1998(04):326-333.
[11] 罗继刚;罗锡辉;李承烈 .[J].石油学报(石油加工),1994,10(03):19.
[12] Biswas J;Bickle G M;Gray P G et al.[J].Catalysis Review-Science and Engineering,1988,30(02):161.
[13] 赵天波;萨学理;汪燮卿 等.[J].石油学报(石油加工),1995,11(02):109.
[14] 陈祥熊;郭文武;高滋 .[J].石油学报(石油加工),1989,5(01):45.
[15] 王娅娟;董玉林;杨孔章 .[J].催化学报,1993,14(04):325.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%