针对攀枝花钢企欣宇化工有限公司精制车间粗TiCl4水解系统运行中存在的问题,在对水解粗TiCl4去除AlCl3机理深入分析的基础上,进行了粗TiCl4的水解沉降实验,研究了被水解的粗TiCl4中固体杂质的最佳含量、水解粗TiCl4的加水量以及沉降时间,讨论分析了上述因素对粗TiCl4中AlCl3去除率的影响。最终得出,控制粗TiCl4水解沉降工艺的关键点为最佳加水量为理论加水量的1.5倍,被水解的粗TiCl4中固体杂质含量最好调整在15~18 g/L,最佳沉降时间为20 h。
There were some problems during the production process of crude titanium tetrachloride hydrolysis and set -tling in the refining workshop in Panzhihua Gangqi Xinyu Chemical Industry Co ., Ltd..The elements like solid impuri-ty content in crude titanium tetrachloride , water volume for hydrolysis , settling time after hydrolysis were researched based on the theory and experiments .The results show that the best water volume is 1.5 times of theoretical volume calculated by the content of aluminum chloride , the solid impurity content prefer to be controlled in the range of 15-18 g/L and the best settling time is 20 h.
参考文献
[1] | 黄子良.精制TiCl4蒸馏釜残液水解回收处理研究[J].钛工业进展,2008(05):35-36. |
[2] | 黄子良.水解在四氯化钛精制中的应用分析[J].钛工业进展,2011(05):38-40. |
[3] | 李慧梅,陈建国,袁玉萍.高含沙浑水在絮凝剂作用下的絮凝沉降试验研究[J].泥沙研究,2006(04):73-77. |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%