简述了粉末注射成形溶剂脱脂的基本过程,介绍了目前使用的一些溶剂脱脂方法及其研究进展,讨论了粉末注射成形溶剂脱脂工艺的发展趋势.

参考文献

[1] German R M.Powder Injection Molding[M].MPIF, Princeton,NJ,1990
[2] Bankovic D R;German R M.Optimization of debinding cycles in Powder Injection Molding[A].MPIF,Princeton, NJ,1990
[3] German R M;Bose Animesh .Injection molding of metals and ceramics[P].US 085406692
[4] 曲选辉;颜寒松;黄伯云 .金属粉末注射成形粘结剂的发展[J].粉末冶金技术,1997,15(01):61.
[5] Li Songlin,Huang Baiyun,Qu Xuanhui,Li Yimin.Solvent de-binding of water-soluble binder in powder injection moulding[J].中国有色金属学会会刊(英文版),1999(03):578-581.
[6] Hwang K S .[J].Rev Particulate Mater,1996,4:71.
[7] Lin S T;German R M .Extraction debinding of Injection Molded parts by condensed solvent[J].Powder Metallurgy International,1989,21(05):19.
[8] Billmeyer F W Jr.Textbook of polymer science[M].New York: John Wiley and Sons Inc,1984:151.
[9] Yang Weiwen;Yang Kaiyuan;Wang Moochin et al.Solvent debinding mechanism for alumina injection molded compacts with water-soluble binders[J].Ceramics International,2003,29:745.
[10] Hosamani Laxmappa .[P].US Pat,0138049,2004.
[11] 李新军,孙红英.粉末注射成形粘结剂及脱脂技术研究进展[J].材料导报,2000(10):56-58.
[12] Jr Wiech .[P].US Pat,4305756,1981.
[13] Johnson K P.Metal injection molding by injectamax process[M].Metal Injection Molding( Ⅱ ). MPIF Princeton,1989:17.
[14] Omar M A;Ibrahim R;Sidik M I et al.Rapid debinding of 316L stainless steel inection moulded component[J].Journal of Materials Processing Technology,2003,140:397.
[15] 范景莲,夏佩华,胡婧,曲选辉,黄伯云,孙玲.钨基高比重钨合金注射坯溶剂脱脂工艺[J].中国有色金属学报,2001(04):651-654.
[16] Ballard C.[J].Cenam Ind,1997(03):42.
[17] Amaya H E .Solvent dewaxing: principles & applic-ation[J].Advances in Powder Metallurgy,1990,3:233.
[18] Rivers R D .[P].US Pat,4113480,1978.
[19] 李益民,黄伯云,曲选辉.当代金属注射成形技术[J].粉末冶金工业,2000(01):14-19.
[20] Lee S H;Jeung Anisotropic W Y .Inection molding of strontium ferrite powder using a PP/PEG binder system[J].Journal of Magnetism and Magnetic Materials,2001,1400:226.
[21] Dowding R J;Rasoul C;Zenger D.Advances in powder metallurgy and particulate materials 1996[J].Princeton,NJ MPIF,1996:15.
[22] 李益民;曲选辉;黄伯云 .金属注射成形的脱脂[J].材料导报,1999,13(01):21.
[23] 李笃信,曲选辉,黄伯云,钟孝贤,李松林,李益民.金属注射成形用新型聚乙二醇基粘结剂的研究[J].稀有金属材料与工程,2001(02):97-100.
[24] Shimizu Toru et al.Supercritical CO2 debinding method in MIM process debindig condition and process in supercritical debinding[J].Journal of the Japan Society of Powder and Powder Metallurgy,1996,43:1188.
[25] Rei M;Milke E C;Gomes R M et al.Low pressure injection molding processing of a 316-L stainless steel feedstock[J].Materials Letters,2002,52:360.
[26] Fleur Bordet et al.The use of co-solvents in supercritical debinding of ceramis[J].Journal of the European Ceramic Society,2002,22:1067.
[27] Mohan;Dirisinghe J E .Fabrication of engineering ceramics by injection molding[J].Ceramic Bulletin,1991,70(05):824.
[28] Kruegur .[P].US 5531958,1996.
[29] 颜鲁婷,司文捷,苗赫濯.CIM中最新脱脂工艺的进展[J].材料科学与工程,2001(03):108-112.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%