采用柠檬酸法制备了SnO2纳米材料,并采用差热-热重、X射线衍射、透射电子显微镜和氮吸附等技术对其进行了表征,考察了其在丙烯醛还原制烯丙醇反应中的催化性能.结果显示,制备的SnO2纳米材料粒径(尺寸为8~10 nm)均一,并具有多孔性质(孔径4~6 nm);在丙烯醛还原制烯丙醇反应中具有良好的催化性能,催化剂的初始活性很高,丙烯醛的初始转化率可达93.6%,烯丙醇的最高选择性为60%,烯丙醇的最高收率为47%.表面结焦是造成催化剂失活的主要原因.
参考文献
[1] | Pederson L R;Maupin G D;Weber W J;McReady D J Stephens R W .[J].Materials Letters,1991,10(9-10):437. |
[2] | Fraigi L;Lamas D G;De Reca N E W .[J].Nanostructured Materiels,1999,11(03):311. |
[3] | Shaji Kumar M D;Srinivasan T M;Ramasamy P;Subramanian C .[J].Materials Letters,1995,25(3-4):171. |
[4] | Chick L A;Pederson L R;Maupin G D;Bates J L Thomas L E Exarhos G J .[J].Materials Letters,1990,10(1-2):6. |
[5] | Juarez R E;Lamas D G;Lascalea G E;De Reca N E W .[J].Journal of the European Ceramic Society,2000,20(02):133. |
[6] | Zhang J R;Gao L .[J].Journal of Solid State Chemistry,2004,177(4-5):1425. |
[7] | Takahashi K;Shibagaki M;Kuno H;Matsushita H .[J].Bulletin of the Chemical Society of Japan,1994,67(04):1107. |
[8] | Bhagwat M;Shah P;Ramaswamy V .[J].Materials Letters,2003,57(9-10):1604. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%