研究以硫酸钪(Sc2(SO4)3)和六次甲基四胺((CH2)6N4)为原料,通过向Sc2(SO4)3溶液中滴加(CH2)6N4溶液,制备出了前驱沉淀物,该前驱沉淀物的化学组成为Sc(OH)2.2(SO4)0.4·0.4H2O,并分析了前驱沉淀物的热分解行为.前驱沉淀物经1100℃煅烧4h后得到了平均粒径为80nm、分散性良好的超细粉体.
参考文献
[1] | 彭超.氧化钪提取新工艺探讨[J].化工设计通讯,2005(02):39-43. |
[2] | Li Jiguang;Ikegami T .[J].Journal of the American Chemical Society,2003,86(09):1493-1499. |
[3] | Hirano M;Kato E .Transformation of Sc O sub 3 -doped tetragonal zirconia polycrystals by aging under hydrothermal conditions[J].Journal of Materials Science,1999(6):1399-1405. |
[4] | KuK C S;Fornasiero L;Mix E et al.[J].Journal of Luminescence,2000,87-89:1122-1125. |
[5] | Fornasiero L.;Peters V.;Petermann K.;Huber G.;Mix E. .New oxide crystals for solid state lasers[J].Crystal Research and Technology: Journal of Experimental and Industrial Crystallography,1999(2):255-260. |
[6] | Kaminskii A A;Bagaev S N;Ueda K et al.[J].Laser Physics Letters,2005,2(01):30-35. |
[7] | 刘颂豪.激光陶瓷--固体激光工作物质探索的新热点[J].激光与红外,2005(06):385-390. |
[8] | Grosso G;Sermon P A .[J].J Matter Chem,2000,10:359-363. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%