从理论上分析了高碳钢方坯连铸中心缩孔产生的原因及降低的途径.通过32炉浇钢试验,得出拉速对中心缩孔的作用大于钢水过热度,同时讨论了强冷段、强冷段水量、二冷段水量等参数对中心缩孔的影响.
参考文献
[1] | Raihle C M .On the Formation of Pipes and Centerline Segregates in Continuously Cast Billets[J].Metallurgical and Materials Transactions,1994,25:123. |
[2] | Sivesson P .Improvement of Inner Quality of Continuously Cast Billets Through Thermal Soft Reduction and Use of Multivariate Analysis of Saved Process Variables[J].Ironmaking and Steelmaking,1996,23(06):504. |
[3] | GABATHULER J P .Fluid Flow into a Dendritic Array Under Forced Convection[J].Metallurgical and Materials Transactions,1983,14:773. |
[4] | 蔡开科.浇注与凝固[M].北京:冶金工业出版社,1987 |
[5] | 陈家祥.炼钢常用图表数据手册[M].北京:冶金工业出版社,1984 |
[6] | 张克强,李永东.方坯高碳钢连铸中心缩孔模型及其应用[J].北京科技大学学报,2001(06):511-513. |