以聚乙二醇(PEG-2000)、甲苯二异氰酸酯(TDI)为原料合成预聚体,然后以3-氨基丙烷乙氧基硅烷(WD-50)对其封端,合成含有柔性链的硅烷偶联剂.并以其为改性剂,用溶胶-凝胶方法制备了EP/SiO2-TiO2 纳米复合材料,利用红外光谱、动态粘弹谱仪、X射线衍射、冲击实验机、扫描电镜和原子力显微镜等手段研究了这种材料的结构与性能.结果表明,与纯环氧树脂相比,改性材料的冲击强度提高了2~3倍,并具有较高的模量和热性能,玻璃化转变温度仅发生微小的变化.
参考文献
[1] | Mimura K. .Improvement of thermal and mechanical properties by control of morphologies in PES-modified epoxy resins[J].Polymer: The International Journal for the Science and Technology of Polymers,2000(12):4451-4459. |
[2] | Tjiong S C;Meng Y Z .[J].Polymer,1999,40:1109-1117. |
[3] | Chiang CL.;Ma CCM. .Synthesis, characterization and thermal properties of novel epoxy containing silicon and phosphorus nanocomposites by sol-gel method[J].European Polymer Journal,2002(11):2219-2224. |
[4] | Kang S;Hong S I I;Choe C R et al.[J].Polymer,2001,42:879-887. |
[5] | Hepburn C.Polyurethane Elastomer[M].Applied Science Publishers,1982:280. |