研究了原位TiC颗粒强化的Fe-26Cr-14Ni基复合材料的常温和高温拉伸性能,分析了该复合材料的断裂特征.结果表明,含5%和10%(体积分数,下同)的TiC复合材料的常温和高温综合拉伸性能明显高于基体合金;TiC含量为10%时具有最佳的高温拉伸性能.随着TiC体积分数的提高,复合材料的常温断裂由韧性断裂向脆性断裂转变.该复合材料的高温断口形貌主要呈现出韧性断裂的特征.
参考文献
[1] | Pandey A B;Mishra R S;Mahajan Y R .Steady State Creep Behavior of Silicon Carbide Particulate Reinforced Alunium Composites[J].Acta Metallurgica Et Materialia,1992,40(08):2045-2052. |
[2] | Park K T;Lavernia E J;Mohamed F A .High Temperature Creep of Silicon Carbide Particulate Reinforecd Aluminum[J].Acta Metallurgica Et Materialia,1990,38(11):2149-2159. |
[3] | 王自东 .接触反应法制备2024/Tic复合材料的微观结构及力学性能[D].哈尔滨工业大学,1994. |
[4] | Hainisi E;Talvitie M;Ristolainen E O .Characterization of Interface Layer between Nitrogen Alloyed Stainless Steel and Alumina in a Metal Matrix Composite[J].Scripta Metallurgica et Materialia,1995,30(10):1333-1336. |
[5] | Skolianos S;Kattamis T Z;Chambers B V .Cast Microstructure and Tribological Properties of Particulate TiC-Reinforced Ni-Base or Stainless Steel Matrix Composites[J].Materials Science and Engineering,1994,183:195-204. |
[6] | Kattamis T Z;Suganuma T .[J].Materials Science and Engineering,1990,128:241252. |
[7] | Terry B S;Chinyamakobvu O S .Dispersion and Reaction of TiC in Liquid Iron Alloys[J].Materials Science and Technology,1992,8(05):399-405. |
[8] | Z.Liu;H.Fredriksson .On the kinetics of carbide precipitation during reaction between graphite and Fe-Ti liquids under microgravity[J].Metallurgical and Materials Transactions, A. Physical Metallurgy and Materials Science,1997(3):707-720. |
[9] | Hui X D;Wang Z F .Structure and Stability of TiC/γ Interface in Fe-Cr-Ni Base Composite[J].Journal of Materials Science and Technology,1999,15(02):151-154. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%