对热浸镀锌层钝化处理可以进一步提高其外观质量和整体防护性能.六价铬对人体和环境有害,传统的六价铬钝化工艺已经被限制使用,并开发了新的代铬(Ⅵ)钝化技术.分别论述了三价铬钝化、无铬钝化及无机盐/有机物复合钝化技术及其机理的研究进展,分析了其优缺点,并指出了未来的发展方向.

参考文献

[1] Roman L;Blidariu M;Cristescu C .Study of conversion coatings on zinc deposition obtained from low pollution solutions[J].Trans IMF,1996,74(05):171-176.
[2] 吴以南.锌镀层的三价铬钝化[J].电镀与环保,2003(02):30-32.
[3] Bellezze T.;Roventi G.;Fratesi R. .Electrochemical study on the corrosion resistance of CrIII-based conversion layers on zinc coatings[J].Surface & Coatings Technology,2002(2/3):221-230.
[4] 蒋建忠,缪树婷,郝利峰,韩生.镀锌层三价铬钝化及钝化膜的封闭处理[J].电镀与涂饰,2013(10):43-46.
[5] 任艳萍,陈锦虹.镀锌层三价铬钝化工艺的研究[J].腐蚀与防护,2007(01):13-16,19.
[6] 夏保佳;杨哲龙;张景双 .锡锌合金镀层钼酸盐及耐蚀性研究[J].表面技术,1993,22(03):108-111.
[7] Treacy GM;Richardson MOW;Wilcox GD .Behaviour of molybdate-passivated zinc coated steel exposed to corrosive chloride environments[J].Journal of Applied Electrochemistry,1999(5):647-654.
[8] 路长青.钼酸盐的缓蚀机理[J].材料保护,1996(10):22.
[9] Twite RL.;Bierwagen GP. .Review of alternatives to chromate for corrosion protection of aluminum aerospace alloys [Review][J].Progress in Organic Coatings: An International Review Journal,1998(2):91-100.
[10] 范云鹰;陈冬华;刘晓晶 等.一种清洁型镀锌件硅酸盐彩色钝化工艺[P].中国,200910094646X,2009-11-18.
[11] 李广超.镀锌层硅酸盐钝化工艺研究[J].电镀与精饰,2007(02):31-33.
[12] Song Y K;Mansefeld F .Development of a molybdate-phosphate-silane-silicate(MPSS) coating process for electro-galvanized steel[J].Corrosion Science,2005,48(01):154-159.
[13] 宫丽,卢燕平,于洋.纳米硅溶胶改性有机复合钝化膜耐蚀性研究[J].表面技术,2004(06):18-20.
[14] Hinton B R W;Wilson L .The corrosion inhibition of zinc with cerous chloride[J].Corrosion Science,1989,29(08):967-985.
[15] Wilson L;Hinton B R W .A method for forming a corrosion coating resistant[P].Australian,WO,006639,1988-09-07.
[16] 张英杰;章江洪;董鹏 等.一种清洁型稀土盐钝化液制备方法[P].中国,200910094371X,2009-09-02.
[17] 朱立群,杨飞.环保型镀锌层蓝色钝化膜耐腐蚀性能的研究[J].腐蚀与防护,2006(10):503-507.
[18] 刘仁志.取代铬酸盐钝化处理工艺的动向[J].全面腐蚀控制,2012(11):40-44.
[19] 左正忠;崔 萍;宋文超 等.镀锌层钛盐钝化的研究[J].电镀与精饰,2010,32(11):9-12.
[20] 郭瑞光,耿志良.无铬转化膜技术研究的几点建议[J].电镀与涂饰,2008(05):38-40.
[21] 卢锦堂,宋进兵,陈锦虹,许乔瑜,孔纲.无铬钝化的研究进展[J].材料保护,1999(03):24-26.
[22] 梁红野,陈彦泽.金属表面植酸钝化处理试验研究[J].石油化工腐蚀与防护,2004(06):5-8.
[23] Paul C. Wynn;Craig V. Bishop .Replacing Hexavalent Chromium[J].Plating & Surface Finishing,2001(2):12-14.
[24] 梁启民;张丽娜.镀锌层单宁酸钝化[J].电镀与精饰,1986(01):31-34.
[25] Van O W J;Zhu D Q .Electrochemical impedance spectroscopy of bis-[3-(triethoxysily) propyl]tetrasulfide on Al 2024-T3 substrates[J].CORROSION,2001,57(05):413-427.
[26] 王楠,徐溢,杨立华,滕毅.硅烷试剂防腐蚀工艺研究[J].材料保护,2001(11):32-33.
[27] 王雪明,李爱菊,李国丽,管从胜.硅烷偶联剂在防腐涂层金属预处理中的应用研究[J].材料科学与工程学报,2005(01):146-150.
[28] Shan F J;Liu C S;Wang S H et al.Corrosion resistance of hot dip galvanized steel pretreated with bis-functional silanes modified with nanoalumina[J].Acta Metall Sin(Eng Lett),2008,21(04):245-250.
[29] Suegama PH;de Melo HG;Recco AAC;Tschiptschin AP;Aoki IV .Corrosion behavior of carbon steel protected with single and bi-layer of silane films filled with silica nanoparticles[J].Surface & Coatings Technology,2008(13):2850-2858.
[30] Montemor M F;Pinto R;Ferreira M O S .Chemical composition and corrosion protection of of silane films mo-dified with CeO2 nanoparicles[J].Electrochimica Acta,2009,54(22):5179-5185.
[31] Deflorian, F.;Rossi, S.;Fedel, M.;Motte, C. .Electrochemical investigation of high-performance silane sol-gel films containing clay nanoparticles[J].Progress in Organic Coatings: An International Review Journal,2010(2):158-166.
[32] Saravanan K;Sathiyanaayanan S;Muralidharan S et al.Performance evaluation of polyaniline pigmented epoxy coating of corrosion protection of steel in concrete environment[J].Progress in organic Coatings,2007,59(02):160-166.
[33] Shi, XM;Nguyen, TA;Suo, ZY;Liu, YJ;Avci, R .Effect of nanoparticles on the anticorrosion and mechanical properties of epoxy coating[J].Surface & Coatings Technology,2009(3):237-245.
[34] 王静,伍林,宋世红,易德莲,黄峰,王娟,陶颖.镀锌层无铬钝化膜耐蚀性能的研究[J].材料保护,2008(11):28-30.
[35] 宫丽,卢琳,卢燕平.薄型无铬有机复合涂层钢板耐蚀性的研究[J].材料保护,2008(02):68-71.
[36] 赵丽虹;李 岩;吴建文 .镀锌板无铬钝化液[P].中国,200710010022.6,2008-07-16.
[37] 宫丽,卢燕平.纳米硅溶胶/丙烯酸复合防蚀薄膜的研究[J].材料保护,2005(01):17-19.
[38] Sohi J;Mcgee J D;Donaldson G T .Passivating composition useful for passivating metal surface,comprises non-ionic or non-ionically stabilized resin in dispersed form,resin consisting of acrylic,polyurethane,vinyl and polyester resins,or their mixtures[P].US,69363-A1,2006-08-03.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%