以牡蛎壳和废玻璃粉为主要原料制备了空心管状型体废水除磷材料,探讨了在500~650℃不同预烧温度、不同样品配方及与废水接触不同时间下样品的废水除磷效果,从而选择最佳制备条件.采用XRD及SEM表征样品的微观结构及组成,采用磷钼蓝分光光度法测定废水中磷的含量.结果表明,含废玻璃粉20%、牡蛎壳80%的样品在600℃煅烧时除磷效果最好,12天后除磷率达到99%;XRD分析显示此时样品主要由3种晶相组成,CaCO3、SiO2和CaO,说明在此温度下牡蛎壳中的部分CaCO3已经分解为CaO.

Hollow cylindric materials for removing phosphate from waste water is prepared in this research.The influences of different calcining temperatures from 500℃ to 650℃ ,different prescription and different contact time on phosphate removal effects are discussed. XRD and SEM techniques are used to investigate the crystals and microstructures. Ammonium phosphomolybdate spectrophotometry method is used to detect the concentration of phosphorous in wastewater. Results show that No. 2 sample with 20% of waste glass powder and 80% of oyster shell powder have the best phosphate remove effect,which can remove 99% of phosphate after contact with waste water for 12 days.XRD shows that 3 crystal phases exist,CaCO3 ,SiO2 and CaO, which suggests that certain amount of CaCO3 decomposed into CaO at this temperature.

参考文献

[1] Morse G K;Lester J N;Perry R .Economic impact of phosphorus removal from wastewater in the european union[J].Eur Water Pollut Control,1994,4:46.
[2] 吴燕,安树林.废水除磷方法的现状与展望[J].天津工业大学学报,2001(01):74-78.
[3] 丁文明,黄霞.废水吸附法除磷的研究进展[J].环境污染治理技术与设备,2002(10):23-27.
[4] 邱菲.凹凸棒石粘土吸附剂除磷酸盐的研究[J].矿产综合利用,1995(05):26.
[5] 王萍.海绵铁除磷技术研究[J].环境科学学报,2000(06):798-800.
[6] S. G. Lu;S. Q. Bai;L. Zhu;H. D. Shan .Removal Mechanism Of Phosphate From Aqueous Solution By Fly Ash[J].Journal of hazardous materials,2009(1):95-101.
[7] 宁平,邓春玲,普红平,牛利民.活性氧化铝吸附水中的磷酸盐[J].有色金属,2002(01):37-39.
[8] 丁文明,黄霞,张力平.水合氧化镧吸附除磷的试验研究[J].环境科学,2003(05):110-113.
[9] 董晓伟,姜国良,李立德,王宁.牡蛎综合利用的研究进展[J].海洋科学,2004(04):62-65.
[10] 陈洁,张吉荣.钼锑抗分光光度法测定水中总磷的探讨[J].仪器仪表与分析监测,2004(03):34-35.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%