以硝酸铋和钛酸四丁酯为原料,以三氯十八烷基硅烷(OTS)为模板,采用自组装单层膜(self-as-sembled monolayers,SAMs)技术,在玻璃基板上成功制备了Bi2Ti2O7晶态薄膜。借助X射线衍射(XRD)、场发射扫描电子显微镜(FE-SEM)、X射线能谱(EDS)及原子力显微镜(AFM)等测试手段对Bi2Ti2O7薄膜进行了表征。结果表明,以OTS为模板利用自组装技术,经540℃煅烧2h可成功制得立方相Bi2Ti2O7晶态薄膜,且薄膜表面平整光滑,均匀致密。

Bi2Ti2O7 thin film was prepared on the glass substrate by the self-assembled monolayer(SAM) tech-nique with Bi(NO3)3 and Ti(OC4H9)4 as the raw materials and octadecyltrichlorosilane as the template.The crystal phase composition,microstructure and topography of the Bi2Ti2O7 thin films were characterized by various techniques,including X-ray diffraction,field-emission scanning electron microscopy,energy disperse spectroscopy and atomic force microscopy.The results indicate the pure cubic phase Bi2Ti2O7 thin film is successfully prepared after annealing at 540℃ for 2h.The prepared Bi2Ti2O7 thin film has a flat,homogeneous and dense surface.

参考文献

[1] Shimada S;Kodaira K;Atsushlta T M .Crystal growth of bismuth titanates and titanium oxide from melts in the system Bi^2 O^3-V^2O^5 TiO^2[J].Journal of Crystal Growth,1977,41(06):317-320.
[2] Fu L W;Wang H;Shang S X et al.Preparation and characterization of Bi^2 Ti^2 O^7 thin films grown by metal organic chemical vapor deposition[J].Journal of Crystal Growth,1994,139(12):319-321.
[3] 肖卓炳,吴显明,王少伟,王弘,王卓,尚淑霞,王民.Bi2Ti2O7薄膜制备及 Bi2Ti2O7绝缘栅场效应管研制[J].功能材料与器件学报,2001(02):171-174.
[4] Wang SW.;Shang SX.;Huang J.;Wang Z.;Wang M.;Wang H. .PZT thin films prepared by chemical solution decomposition using a Bi2Ti2O7 buffer layer[J].Journal of Crystal Growth,2000(4):388-392.
[5] Wenbiao W;Keigo F;Yoshihiro O et al.Bismuth titanate thin films on Si with buffer layers prepared by laser ablation and their electrical properties[J].Japanese Journal of Applied Physics,1996,35(07):1560-1563.
[6] Wang H;Fu L W;Shang S X et al.The influence of substrate temperature and annealing on phase formation and crystal line properties of bismuth titanate films by APMOCVD[J].Journal of Physics D:Applied Physics,1994,27(03):393-395.
[7] Kuniki Y;Minoru I;Soiehiro O et al.Preparation of ferroelectric Bi^4 Ti^3 O^12 thin films with c-axis orientation by atmospheric-pressure metalorganic chemical vapor deposition[J].Japanese Journal of Applied Physics,1995,34(02):2425-2429.
[8] 林元华,王建飞,何泓材,周剑平,周西松,南策文.脉冲激光沉积法合成Bi2Ti2O7介电薄膜及其光吸收特性[J].半导体学报,2005(z1):74-77.
[9] 王少伟,陆卫,王弘,王栋,王民,沈学础.Bi2 Ti2 O7/Si薄膜的制备及C-V特性研究[J].物理学报,2001(12):2461-2465.
[10] 杨生荣,任嗣利,张俊彦,张绪寿.自组装单分子膜的结构及其自组装机理[J].高等学校化学学报,2001(03):470-476.
[11] Gao YF;Koumoto K .Bioinspired ceramic thin film processing: Present status and future perspectives[J].Crystal growth & design,2005(5):1983-2017.
[12] 谈国强,任宣儒,苗鸿雁.退火工艺对液相自组装法制备BiFeO3薄膜的影响[J].功能材料,2011(02):373-375.
[13] 刘剑,谈国强,苗鸿雁,贺中亮,夏傲.OTS自组装单层膜诱导定向生长SrTiO3功能陶瓷薄膜[J].无机化学学报,2009(03):517-521.
[14] 谈国强,博海洋,苗鸿雁,夏傲,贺中亮.BiFeO3薄膜的液相自组装制备与表征[J].无机材料学报,2010(01):83-86.
[15] 谈国强,刘剑,苗鸿雁,贺中亮,夏傲.四方相BaTiO3薄膜的自组装制备与表征[J].无机材料学报,2009(04):749-754.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%