在不同流延条件下制备聚丙烯(PP)流延基膜,并对基膜施加拉伸使其形成微孔,通过差示扫描量热测试和傅立叶变换红外光谱表征基膜的结晶度、片晶厚度和晶区的取向程度等硬弹性结构参数,使用扫描电镜观察微孔膜的孔形态并测定了微孔膜的透气率,研究了流延工艺条件与基膜的硬弹性结构及拉伸成孔性之间的关系.结果表明,流延辊温度主要影响基膜结晶度和片晶厚度,牵伸比主要影响晶区取向程度.基膜硬弹性结构越完善,弹性回复率越大,拉伸后形成的微孔数量越多,孔形态和孔结构更加均匀,透气率增大.

参考文献

[1] Tabatabaei, SH;Carreau, PJ;Aji, A .Structure and properties of MDO stretched polypropylene[J].Polymer: The International Journal for the Science and Technology of Polymers,2009(16):3981-3989.
[2] Jianlin Li;Claus Daniel;David Wood .Materials processing for lithium-ion batteries[J].JOURNAL OF POWER SOURCES,2011(5):2452-2460.
[3] Farhad Sadeghi;Abdellah Ajji;Pierre J. Carreau .Analysis of microporous membranes obtained from polypropylene films by stretching[J].Journal of Membrane Science,2007(1/2):62-71.
[4] Farhad Sadeghi;Abdellah Ajji;Pierre J. Carreau .Analysis of Row Nucleated Lamellar Morphology of Polypropylene Obtained From the Cast Film Process: Effect of Melt Rheology and Process Conditions[J].Polymer engineering and science,2007(7):1170-1178.
[5] Tabatabaei, SH;Carreau, PJ;Ajji, A .Effect of processing on the crystalline orientation, morphology, and mechanical properties of polypropylene cast films and microporous membrane formation[J].Polymer: The International Journal for the Science and Technology of Polymers,2009(17):4228-4240.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%