以合成的微孔分子筛MCM-22为原料,将其与表面活性剂及氢氧化钠一起回流溶解,再调节溶液的pH值至7~9, 使MCM-22转化为高水热稳定性的介孔材料. 所得介孔材料具有蠕虫状的均匀孔道,骨架中不含有MCM-22的微观结构单元. 该介孔材料至少含有18%的表面活性剂,经823 K焙烧脱除表面活性剂后,其孔径为2 2 nm, 比表面积为 1 038 m2/g, 孔容为0 97 cm3/g. 焙烧后的介孔材料具有非常高的水热稳定性,经沸水回流100 h后其比表面积为896 m2/g, 孔容为0 90 cm3/g, 孔径为2 1 nm, 即使经过300 h的回流,该材料仍能保持698 m2/g的比表面积和0 90 cm3/g的孔容. 固体 29Si MAS NMR结果表明,该介孔材料的高水热稳定性与其高表面缩合度有关.
参考文献
[1] | Liu Y.;Pinnavaia TJ.;Zhang WZ. .Steam-stable aluminosilicate mesostructures assembled from zeolite type Y seeds[J].Journal of the American Chemical Society,2000(36):8791-8792. |
[2] | Liu Y;Zhang W Zh;Pinnavaia T J .[J].Angewandte Chemie International Edition,2001,40(07):1255. |
[3] | Zhang Z T;Han Y;Zhu L;Wang R W Yu Y Qiu Sh L Zhao D Y Xiao F-S .[J].Angewandte Chemie International Edition,2001,40(07):1258. |
[4] | Zhang Z T;Han Y;Xiao F-S;Qiu Sh L Zhu L Wang R W Yu Y Zhang Z Zou B S Wang Y Q Sun H P Zhao D Y Wei Y .[J].Journal of the American Chemical Society,2001,123(21):5014. |
[5] | Han Y;Xiao F S;Wu Sh;Sun Y Y Meng X J Li D Sh Lin S Deng F Ai X J .[J].Journal of Physical Chemistry B,2001,105(33):7963. |
[6] | Han Y.;Wu S.;Sun YY.;Li DS.;Xiao FS.;Liu J.;Zhang XZ. .Hydrothermally stable ordered hexagonal mesoporous aluminosilicates assembled from a triblock copolymer and preformed aluminosilicate precursors in strongly acidic media[J].Chemistry of Materials,2002(3):1144-1148. |
[7] | 刘子玉,刘中民,齐越,许磊,何艳丽,杨越,张阳阳.凝胶硅铝比对合成MCM-22,UTM-1和Kenyaite的影响[J].催化学报,2004(07):542-546. |
[8] | Liu, ZY;Wei, YX;Qi, Y;Zhang, SG;Zhang, Y;Liu, ZM .Synthesis of MCM-41 type materials with remarkable hydrothermal stability from UTM-1[J].Microporous and Mesoporous Materials,2006(1/3):205-211. |
[9] | Liu Z Y;Wei Y X;Qi Y;Sang Sh Y Liu Zh M .[J].Studies in Surface Science and Catalysis,2007,165:41. |
[10] | Rubin M K;Chu P .[P].US 4954325,1990. |
[11] | Ryoo R;Kim J M;Ko C H;Shin C H .[J].Journal of Physical Chemistry,1996,100(45):17718. |
[12] | Imae T;Kohsaka T .[J].Journal of Physical Chemistry,1992,96(24):10030. |
[13] | Cassidy M A;Warr G G .[J].Journal of Physical Chemistry,1996,100(08):3237. |
[14] | Corma A;Corell C;Fornes V;Kolodziejski W Perez-Pariente J .[J].Zeolites,1995,15(07):576. |
[15] | 许海红,郭岱石,蒋淇忠,马紫峰,李婉君,王铮.硫酸根促进的纯硅MCM-41催化假性紫罗兰酮环化合成紫罗兰酮的性能[J].催化学报,2006(12):1080-1086. |
[16] | 史建公,卢冠忠,曹钢,于晓东.MCM-22分子筛的稳定性研究[J].石油化工,2006(10):948-952. |
[17] | Corma A;Navarro M T;Perez-Pariente J.[J].Journal of the Chemical Society,Chemical Communications,1994(02):147. |
[18] | Blasco T.;Navarro MT.;Pariente JP.;Corma A. .SYNTHESIS, CHARACTERIZATION, AND CATALYTIC ACTIVITY OF TI-MCM-41 STRUCTURES[J].Journal of Catalysis,1995(1):65-74. |
[19] | Cheng M J;Tan D L;Liu X M;Han X W Bao X H Lin L W .[J].Microporous and Mesoporous Materials,2001,42(2-3):307. |
[20] | Marques A L S;Monteiro J L F;Pastore H O .[J].Microporous and Mesoporous Materials,1999,32(1-2):131. |
[21] | 彭建彪,谢素娟,徐龙伢,王清遐.MCM-22 分子筛的结构、性质及合成和应用前景[J].天然气化工,2001(02):42-47. |
[22] | Leu CM.;Wu ZW.;Wei KH. .Synthesis and properties of covalently bonded layered silicates/polyimide (BTDA-ODA) nanocomposites[J].Chemistry of Materials,2002(7):3016-3021. |
[23] | Mokaya R .[J].Journal of Physical Chemistry B,1999,103(46):10204. |
[24] | Inagaki S;FukushimaY;Kuroda K .[J].Studies in Surface Science and Catalysis,1994,84:125. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%