欢迎登录材料期刊网

材料期刊网

高级检索

以Ca(NO3)2和(NH4)2HPO4为原料,应用超声化学法制备得到了尺寸约20nm×120nm、分散性良好的针状羟基磷灰石(HAp)纳米粉体.对比研究了超声化学法与传统的化学沉淀法对HAp粉体的结晶性能、Ca/P摩尔比和产率的影响.研究表明,与传统的化学沉淀法相比,超声化学法可以在较短的时间内显著地提高纳米HAp的合成效率、结晶度、Ca/P摩尔比和产率.

参考文献

[1] Suslick K S .Sonochemistry[J].Science,1990,247:1439.
[2] Thomopson L H;Doraiswamy L K .Sonochemistry:science and engineering[J].Industrial and Engineering Chemistry Research,1999,38:1215.
[3] Mason TJ .Ultrasound in synthetic organic chemistry[J].Chemical Society Reviews,1997(6):443-451.
[4] Bhatkhande B S;Samant S D .Sonochemical chloro-oxidation of pHenols using HCl-H2O2[J].Ultrasonics Sonochemistry,1998,5(07)
[5] Okitsu K;Mizukoshi Y;Bandow H .Synthesis of palladium nanoparticles with interstitial carbon by sonochemical reduction of tetrachloropalladate(Ⅱ)in aqueous solution[J].Journal of Physical Chemistry B,1997,101:5470.
[6] 李春喜,王子镐.超声技术在纳米材料制备中的应用[J].化学通报,2001(05):268-271,267.
[7] Mdleleni MM.;Suslick KS.;Hyeon T. .Sonochemical synthesis of nanostructured molybdenum sulfide[J].Journal of the American Chemical Society,1998(24):6189-6190.
[8] 邱晓峰,朱俊杰.超声化学制备单分散金属纳米钯[J].无机化学学报,2003(07):766-770.
[9] 沈国柱,徐政,朱英杰.不同形貌ZnO纳米粒子的超声化学法制备与表征[J].无机化学学报,2005(06):893-896.
[10] 沈国柱,徐政.超声化学法在纳米材料制备中的应用[J].材料导报,2004(z1):12-14,18.
[11] 孙静,高濂,郭景坤.分散剂用量对几种纳米氧化锆粉体尺寸表征的影响[J].无机材料学报,1999(03):465-469.
[12] 华缜,靳正国,程志捷.超声条件下羟基磷灰石纳米针状晶体的制备[J].材料导报,2003(z1):75-77.
[13] 王英,靳正国,华缜,程志捷.超声处理对羟基磷灰石纳米针状晶形成的影响[J].硅酸盐通报,2003(06):24-26,38.
[14] Peters F.;Epple M.;Schwarz K. .The structure of bone studied with synchrotron X-ray diffraction, X-ray absorption spectroscopy and thermal analysis[J].Thermochimica Acta: An International Journal Concerned with the Broader Aspects of Thermochemistry and Its Applications to Chemical Problems,2000(1/2):131-138.
[15] Liu C;Huang Y;Shen W;Cui J .Kinetics of hydroxyapatite precipitation at pH 10 to 11.[J].Biomaterials,2001(4):301-306.