介绍了Ni3Al基金属间化舍物研究的现状和前景.由于Ni3Al基金属间化合物具有高熔点、低密度和良好的抗氧化性等性能,长期以来作为高温结构的候选材料而得到了广泛的关注,但是Ni3Al在室温下塑性差和高温时强度低限制了它的使用.采用合金化的方法可使Ni3Al基金属间化合物的性能得到改善,着重介绍了合金元素在Ni3Al基金属间化合物中的作用.
参考文献
[1] | Chowdhury S G J et al.[J].INTERMETALLICS,2007,15:260. |
[2] | Chen Guoliang;Ni Xiaodong;Timothee Nsongo .[J].Interrnetal-lics,2004,12:733. |
[3] | Soga W et al.[J].Intermetallics,2006,14:170. |
[4] | Jozwik P.;Jezierska E.;Bojar Z. .TEM investigations of Ni3Al-based intermetallic polycrystals[J].Materials Chemistry and Physics,2003(2/3):448-451. |
[5] | Shibuya S et al.[J].Acta Materials,2006,54:861. |
[6] | Ismail R;Yaacob I I .[J].Journal of Alloys and Compounds,2005,392:214. |
[7] | Lee Dongyun;Santella M L;Anderson I M .[J].Intermetallics,2005,13:187. |
[8] | 梅炳初,王为民,袁润章.Ni3Al的有序性、脆性及塑性[J].武汉工业大学学报,1996(01):1-4. |
[9] | Chiba A;Hanada S .[J].Scripta Metallurgica,1989,25:1883. |
[10] | Ges A M et al.[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2007,458:96. |
[11] | Seiji Miura;Satoshi Takizawa;Tomoo Suzuki .Effect of tetragonal distortion introduced by anti-site defect configuration on additional hardening in off-stoichiometric Al-rich Ni_3Al alloys[J].Acta materialia,2005(19):5175-5181. |
[12] | Souza N D;Dong H B .[J].Scripta Materialia,2007,56:41. |
[13] | Hello Goldenstein;Yuri Nunes Silva;Humberto N Yo-shimura .[J].Intermetallics,2004,12:963. |
[14] | 陈国良.有序金属化合物结构材料物理金属学基础[M].北京:冶金工业出版社,1999 |
[15] | Zhu J;Cao W;Yang Y .[J].Acta Materials,2007,55:4545. |
[16] | Paidar V;Pope D P;Vitek V .[J].Acta Metallurgy,1984,32(03):435. |
[17] | 彭超群,黄伯云,贺跃辉.Ni-Al系、Fe-Al系和Ti3Al金属间化合物研究进展[J].特种铸造及有色合金,2001(06):27-29. |
[18] | Yong Ma;Alan J. Ardell .Coarsening of gamma (Ni-Al solid solution) precipitates in a gamma' (Ni_3Al) matrix[J].Acta materialia,2007(13):4419-4427. |
[19] | Satoshi Takizawa;Seiji Miura;Tetsuo Mohr .[J].Intermetallics,2005,13:1137. |
[20] | 冯涤,李尚平,骆合力,张春福,陈蓓京.改性铸造Ni3Al基合金MX246组织与性能研究[J].金属学报,2002(11):1181-1185. |
[21] | Lapin J .[J].Intermetallics,2006,14:1417. |
[22] | Merabtine R et al.[J].Intermetallics,2005,13:179. |
[23] | Shibuya S et al.[J].INTERMETALLICS,2007,15:119. |
[24] | Lee Dongyun et al.[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2006,428:196. |
[25] | Nunomura Y et al.[J].Intermetallics,2004,12:389. |
[26] | 张迎九;谢佑卿 .李为民[J].金属学报,1996,32(05):479. |
[27] | 陈金栌,朱定一,林登宜.Ni3Al基合金的研究与应用进展[J].材料导报,2006(01):35-38. |
[28] | 李玉芳,郭建亭,周兰章,叶恒强.Ni3Al(Z)合金室温拉伸性能及Zr韧化机制的探讨[J].稀有金属材料与工程,2004(10):1061-1064. |
[29] | Liu C T;Sticgler J O .[J].Materials and Engineering,1984,100(05):129. |
[30] | Takasugi T et al.[J].ACTA METALLURGICA,1985,33(07):1259. |
[31] | Chantal K. Sudbrack;Ronald D. Noebe;David N. Seidman .Compositional pathways and capillary effects during isothermal precipitation in a nondilute Ni-Al-Cr alloy[J].Acta materialia,2007(26):119-130. |
[32] | George EP.;Lin H.;Pope DP.;Liu CT. .ENVIRONMENTAL EMBRITTLEMENT AND OTHER CAUSES OF BRITTLE GRAIN BOUNDARY FRACTURE IN NI3AL[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,1995(0):277-288. |
[33] | Wu YX;Li XY;Wang YM .First-principles study of the influence of lattice misfit on the segregation behaviors or hydrogen and boron in the Ni-Ni3Al system[J].Acta materialia,2007(14):4845-4852. |
[34] | Chantal K Sudbrack;Kevin E Yoon;Ronald D Noebe .[J].Acta Materialia,2006,54:3199. |
[35] | 袁泽喜;宋申华;习天辉 .[J].武汉钢铁学院学报,1994,17(04):375. |
[36] | 何玉怀,刘绍伦,赵希宏.Ni3Al合金热/机械疲劳裂纹扩展速率试验及其预测研究[J].航空动力学报,2002(01):93-96. |
[37] | Lapin J.[J].Intermetallics,1999(07):599. |
[38] | 孙岩,刘瑞岩,张俊善,祝美丽.NiAl基金属间化合物的研究进展[J].材料导报,2003(07):10-13. |
[39] | Lu Yuxiang;Chen Weixing;Reg Eadie .[J].Intermetallics,2004,12:1299. |
[40] | 李树索,韩雅芳,肖程波,宋尽霞.Ni3Al基合金IC6及MCrAlY包覆涂层的抗腐蚀性能[J].中国有色金属学报,2003(06):1451-1455. |
[41] | 肖程波,韩雅芳.硅对定向凝固Ni3Al基合金IC6A微观组织和性能的影响[J].稀有金属材料与工程,2003(08):670-673. |
[42] | Izumi T;Mu N;Zhang L;Gleeson B .Effects of targeted gamma-Ni plus gamma '-Ni3Al-based coating compositions on oxidation behavior[J].Surface & Coatings Technology,2007(4/7):628-631. |
[43] | Lee D B;SanteUa M L .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2004,374:217. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%