研究了液相线半连续铸造法制备A356铝合金半固态浆触变成形并经固溶时效处理后的组织与性能.结果表明,触变成形与热处理后的A356件,其σb值达到238MPa,δ5达到17%,此结果为液相线半连续铸造A356铝合金触变成形的深入研究奠定了基础.
参考文献
[1] | Kirkwood D H;Kapranos P .Semi solid Processing of Alloy[J].Metals and Materials,1988,11(02):16. |
[2] | Flemings M C;Piek R G;Young K P .The Theology of a Partially Solid Alloy[J].Metallurgical and Materials Transactions,1972,17(03):1925-1932. |
[3] | Fleming M C .Behavior of Metal Alloys in the Semi solid State[J].Metallurgical and Materials Transactions,1991,22(06):269. |
[4] | 陈晓阳 et al.[J].中国有色金属学报,2000(11):728. |
[5] | Kirkwood D H .[J].International Metals Reviews,1994,39(05):173. |
[6] | Chiarmetta G.Thixoforming of Automobile Components[A].Shetlied:The University of Sheffield,1996:204-207. |
[7] | Nakada Masayuki;Shiohara Yuh;Flemings M C .Semi solid Processing of Copper Alloys for Electric Motor Components[J].(Si)International,1990,30(01):27. |
[8] | 崔建忠,路贵民,刘丹.半固态浆制备技术的新进展[J].哈尔滨工业大学学报,2000(04):110. |
[9] | 周鸿章 et al.[J].稀有金属材料与工程,2001(30):87. |
[10] | 路贵民,董杰,崔建忠.7075合金液相线半连续铸造与二次加热的合金组织[J].中国有色金属学报,2001(02):211-2156. |
[11] | Chen CP.;Tsao CYA. .RESPONSE OF SPRAY-DEPOSITED, STIRRED-CAST AND CONVENTIONAL CAST PB-SN ALLOYS TO DEFORMATION IN THE SEMI-SOLID STATE[J].Journal of Materials Science,1995(16):4019-4026. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%