采用浸渍法制备了CuO-NiO/SiO2负载型催化剂. 以空气为氧源,对CuO-NiO/SiO2催化体系催化氧化1-甲氧基-2-丙醇合成甲氧基丙酮反应的催化活性进行了考察. 实验结果表明,NiO组分的负载量对催化活性影响较大; NiO和CuO两者之间有很强的协同催化效应. TPR和XRD结果表明,添加镍组分可促进铜在载体表面上分散,使氧化物还原温度降低,提高催化活性. 在优化条件下,1-甲氧基-2-丙醇的转化率可达74.3%,甲氧基丙酮的收率可达63%.
参考文献
[1] | Venturello C;Ricci M .[J].Journal of Organic Chemistry,1986,51(09):1599. |
[2] | Mariella R P;Leech J L .[J].Journal of the American Chemical Society,1949,71(10):3558. |
[3] | Mallat T;Baiker A .[J].Applied Catalysis A:General,1991,79(01):41. |
[4] | Mallat T;Baiker A .Patscheider J[J].Applied Catalysis A:General,1991,79(01):59. |
[5] | Mallat T;Baiker A;Botz L .[J].Applied Catalysis A:General,1992,86(02):147. |
[6] | HayashiH;Kikawa K;Murai Y;Shigemoto N Sugiyama S Kawashioro K .[J].Catalysis Letters,1996(36):99. |
[7] | 王军伟,周宁,赵春霞,曹国英,胡信全,HU Xinquan.添加物对1-甲氧基-2-丙醇催化氧化制甲氧基丙酮反应的影响[J].催化学报,2001(01):87-88. |
[8] | Friedli H R[P].US 3462495,1969. |
[9] | Landau M V;Kogan S B;Herskowitz M .[J].Studies in surface science and catalysis,1997,108:407. |
[10] | Stansbury H A Jr;Decker H J .[P].US 3625836,1971. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%