利用电化学方法和化学分析技术,研究了工业纯钛(TAl)在卤化物水溶液中钝化膜的破裂行为.提出了卤素在钝化膜表面的局部析出阻碍了膜的生长并在电场力的作用下导致破膜的观点,较好地解释了实验结果.
The electrochemical measurement and chemical analytical techniques are used to study the behaviour of passivity breakdown of commercial pure Ti in halide aqueous solutions.The results show that the passivity breakdown of titanium is closely related to the
参考文献
[1] | AbdRabbohMF,BobenPJ.InProceedingsofInternationalConferenceonLocalizedCorrosion,NACE,Houston,1974,653.2CasillasN,CharleboisSJJElectrochem.Soc,1994,141(3):636.3张新革,火时中.腐蚀科学与防护技术,1992,4(4):2294Szklarska-SmialowskaZ.PittingCorrosionofMetals,NACE,Houston,1986,2335森冈进,梅园昭已.日本金属学会志,1959,23:188.6MansfeldF.Electrochem.Soc.,1971,118(9):1412.7NishimuraR,KudoK.Corros.Sci.,1982,22(7):637.8《无机化学》编写组编.无机化学(下册)北京:人民教育出版社,1978.44.9裴润等编.硫酸法钛白生产.北京:化学工业出版社,1982.4 |