依据Murakami的“夹杂物等效投影面积模型”估算了在高周疲劳条件下一定硬度(或强度)高强钢的“临界夹杂物尺寸”. 估算结果表明, 随着钢硬度(或强度)的增加, “临界夹杂物尺寸”逐渐减小; “临界夹杂物尺寸”也受构件表面机加工粗糙度的影响, 表面越光洁, 这个尺寸也越小.从本文几种钢的实验数据以及其它已发表的数据都可以间接证明, 估算的临界尺寸是合理的
The critical inclusion sizes (CIS) of some steels with given matrix hardness or tensile strength and surface roughness under high cycle fatigue condition were estimated mainly on the basis of Murakami's theory, i.e., the inclusion equivalent projected area model. The results show that the CIS decreases with increasing Vickers hardness (or tensile strength) and decreasing surface roughness of specimen. The estimated CIS is supported indirectly by the experimental data from present study and previous publications available.