欢迎登录材料期刊网

材料期刊网

高级检索

Strontium bismuth tantalum (SBT) fine power was prepared by Sol-Gel method. Pentaethoxy tantalum, strontium acetate and bismuth subnitrate were used as raw materials, and were dissolved in proper order in ethylene glycol to form transparent sol. The mixed precursor was dried at 80℃ and annealed at 800℃ for 1 h. Crystallized nanometer sized SBT fine powder was obtained and characterized by XRD.