The glass-ceramic was prepared on the basis of materials of granulated slag containing high-calcium oxide and cullet.The content of granulated slag ranges from 50%-60%wt in the glass compositions. The samples were analyzed by DTA, SEM and XRD.The results show that the main crystal phase of the glass-ceramic is β-CaSiO3,Which is in scattering fiber or column form.The applying properties have also been measured.
参考文献
[1] | Tang Shaoqiu;Liang zhongjun.Study on Antimony Slag Glass-Ceramic[J].Bulletin of the Chinese Ceramic Society(in Chinese),1994(02):18-24. |
[2] | MIYUKI HAYASHI;MASAHIRO SUSA;TOSHIO MARUYAMA;KAZUHIRO NAGATA .Phase and Magnetic Properties of Iron Oxide Clusters in 20CaO·20SiO_2·7Fe_2O_3·6FeO Glasses[J].Journal of Electronic Materials,1995(8):983-989. |
[3] | Satyabrata Ray;Muchow G M .Preparation Glass-ceramic based on Cullet and Waste Residue[J].Journal of the American Ceramic Society,1989,51(12):678-682. |
[4] | Wang Chenyu;Hao Yanwu;Tao Ying .Influence of Amount of Nucleating Agent on Properties of Wolfram Tailing Glass-Ceramic[J].Glass,1994,21(05):1-5. |
[5] | Krystyna E;Linpinska-Kalita;Edward Gorlich .On the Valence State and Coordiantion of Iron Cations in Alumino-silicate Glasses[J].Journal of Non-Crystalline Solids,1988,107:73-80. |
[6] | Wang Changwen;Sheng Shulan .Glass Ceramic with Low Expansion Coefficients[J].武汉理工大学学报,1989,16(02):23-27. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%