采用放电等离子烧结的方法制备出Fe67Co9.5Nd3Dy0.5B20大块非晶合金,且具有很好的非晶性能.用DTA热分析得到合金的第一次晶化结束温度为650℃.在650℃下保温10min退火热处理后,合金出现了较好硬磁性,合金的最大磁能积达61kJ/m3,粉末颗粒的大小对合金的磁性能影响不大.Nd1.1Fe4B4相的析出也对矫顽力有一定影响.
参考文献
[1] | Coehoorn R;de Mooij B;Duchateau J P W B et al.[J].J de Phys Colloque,1988,49C8:669-670. |
[2] | Kneller E.F.;Hawig R. .The exchange-spring magnet: a new material principle for permanent magnets[J].IEEE Transactions on Magnetics,1991(4):3588-3560. |
[3] | Kanekiyo H.;Uehara M. .Microstructure and magnetic properties of high-remanence Nd/sub 5/Fe/sub 71.5/Co/sub 5/B/sub 18.5/M (M=Al, Si, Ga, Ag, Au) rapidly solidified and crystallized alloys for resin-bonded magnets[J].IEEE Transactions on Magnetics,1993(6):2863-2865. |
[4] | Manaf A;Buckley R A;Davis H A .[J].Journal of Magnetism and Magnetic Materials,1993,128:302-306. |
[5] | Takahashi N;Sugimoto S;Okada M et al.[J].Trans IEEE Japan,1993,113-A:251-260. |
[6] | Mishra R K;Panchanathan V .[J].Journal of Applied Physics,1994,75:6652-6654. |
[7] | Withanawasam L;Murphy A S;Hadjipanayis G C et al.[J].Journal of Applied Physics,1994,76:7065-7067. |
[8] | Inoue A;Takeuchi A;Makino A et al.[J].Materials Transactions-Japan Institute of Metals,1995,36:676-685. |
[9] | Raviprasad K.;Umemoto M.;Funakoshi M. .Synthesis and characterization of Nd2Fe14B-25 vol % Fe nanocomposite magnets[J].Journal of Applied Physics,1998(2):921-929. |
[10] | Kawamura Y;Shibata T;Inoue A et al.[J].Scripta Metallurgica Et Materialia,1997,37:431-436. |
[11] | Kawamura Y;Inoue A;Nakamura T .Superplasticity in Pd sub 40 Ni sub 40 P sub 20 metallic glass[J].Materials Science Forum,1999(0):349-354. |
[12] | Kawamura Y;Nakamura T;Inoue A et al.[J].Materials Transactions Jim,1999,40:794-803. |
[13] | Kawamura Y;Takagi M;Akai M et al.[J].Materials Science and Engineering,1988,98:449-452. |
[14] | Kawamura Y;Inoue A;Masumoto T .[J].Scripta Metall,1993,29:25-30. |
[15] | Kawamura M;Takagi M;Senoo M et al.[J].Materials Science and Engineering,1988,98:415-418. |
[16] | Takagi M;Kawamura Y;Imura T et al.[J].Journal of Materials Science,1992,27:956-962. |
[17] | Raybould D;Tan K S .[J].Journal of Materials Science,1985,20:2776-2786. |
[18] | Esaki H;Ameyama K;Tokizane M .[J].Materials Science and Technology,1989,5:369-376. |
[19] | Kawamura Y;Inoue A;Kojima A et al.[J].Journal of Applied Physics,1994,76:5545-5551. |
[20] | Cline C F;Hopper R W .[J].Scripta Metall,1977,11:1137-1138. |
[21] | Pruemmer R .[J].Materials Science and Engineering,1988,98:461-463. |
[22] | Morris D G .[J].Journal of Materials Science,1982,17:1789-1794. |
[23] | Kasiraj P;Dostka D;Vreeland T et al.[J].J Non-Cryst Sol,1984,61-62:967-972. |
[24] | Kawamura Y;Kato H;Inoue A et al.[J].Applied Physics Letters,1995,67:2008-2010. |
[25] | Kawamura Y;Kato H;Inoue A et al.[J].International Journal of Powder Metallurgy,1997,33:50-61. |
[26] | Itoi T;Takamizawa T;Kawamura Y et al.[J].Scripta Materialia,2001,45:1131-1137. |
[27] | Yoshida S;Mizushima T;Makino A et al.[J].Journal of The Japan Institute of Metals,1999,63:1097-1100. |
[28] | Shen B;Kimura H;Inoue A et al.[J].J Jpn Soc Powder Powder Metall,2001,48:858-862. |
[29] | Zhang W;Fujita K et al.[J].Materials Transactions Jim,1999,40:1123-1129. |
[30] | Zhang W;Inoue A .[J].Applied Physics Letters,2002,80:1610-1612. |
[31] | Zhang W.;Inoue A. .Influence of ribbon thickness on the formation and magnetic properties of melt-spun Fe-Co-Nd-Dy-B metallic glasses[J].Journal of Applied Physics,2001(2):1509-1511. |
[32] | Ishihara S;Zhang W .[J].MATERIALS TRANSACTIONS,2003,44:138-143. |
[33] | 黄永杰.非晶态磁性物理与材料[M].成都:电子科技大学出版社,1991:118. |
[34] | Zhang W.;Inoue A.;Matsushita M. .Hard magnetic properties of Fe-Co-Nd-Dy-B nanocrystalline alloys containing residual amorphous phase[J].Journal of Applied Physics,2001(1):492-495. |
[35] | Stoner E C;Wohlfarh E P .[J].Philos Trans R Soc London Se,1948,A240:599-604. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%