参考文献
[1] | 尹开锯,李聪,邱绍宇等.核废料包装材料研究现状[J].核动力工程,2007,28(2):76 |
[2] | 王驹,陈伟明,苏锐等.我国高放废物地质处置库场址筛选总体技术思路探讨[J].世界核地质科学,2011,28(1):45 |
[3] | Bennett D G,Gens R.Overview of European concepts for high-level waste and spent fuel disposal with special reference waste container corrosion[J].J.Nucl.Mater.,2008,379:1 |
[4] | Féron D,Crusset D,Gras J M.Corrosion issues in nuclear waste disposal[J].J.Nucl.Mater.,2008,379:16 |
[5] | Johnson L H,Shoesmith D W,Ikeda B M,et al.Lifetimes of titanium and copper containers for the disposal of used nuclear fuel[J].Mat.Res.Soc.Symp.Proc,1992,257:439 |
[6] | Shoesmith D W,Hocking W H,Ikeda B M,et al.Application of electrochemical methods in the development of models for fuel dissolution and container corrosion under nuclear waste disposal conditions[J].Can.J.Chem.,1997,75:1566 |
[7] | Nakayama G,Sakakibara Y,Taniyama Y,et al.The long-term behaviors of passivation and hydride layer of commercial grade pure titanium in TRU waste disposal environments[J].J.Nucl.Mater.,2008,379:174 |
[8] | Nishimura T,Corrosion resistance of molybdenum-containing titanium alloy for overpack in simulating underground environment[J].J.Nucl.Mater.,2009,385(3):495 |
[9] | He X,No(e)l J J,Shoesmith D W.Temperature dependence of crevice corrosion initiation on titanium grade-2[J].J.Electrochem.Soc.,2002,149(9):B440 |
[10] | Mckay P,Mitton D B.An electrochemical investigation of localized corrosion on titanium in chloride environments[J].Corrosion,1985,41(1):52 |
[11] | He X,No(e)l J J,Shoesmith D W.Effects of iron content on microstructure and crevice corrosion of grade-2 titanium[J].Corrosion,2004,60(4):378 |
[12] | Tsujikawa S,Kojima Y.Repassivation method to predict long term integrity of low alloy titanium for nuclear waste package[J].Mater.Res.Soc.Symp.Proc,1991,212:261 |
[13] | 郭永海,王驹,刘淑芬等.高放废物处置库预选区野马泉岩体地下水化学特征[J].原子能科学技术,2004(38增刊):143 |
[14] | 阳靖峰.高放废物地质处置环境下金属处置罐材料的腐蚀行为[D].中国科学院,2011 |
[15] | Andresen P L,Gordon G M,Lu S C.The stress-corrosion-cracking model for high-level radioactive-waste packages[J].JOM-Min.Met.Mat.,2005,1S:27 |
[16] | Griess J C.Crevice corrosion of titanium in aqueous salt solutions[J].Corrosion,1968,24(4):96 |
[17] | R.温斯顿.里维.尤利格腐蚀手册[M].北京:化学工业出版社,2005 |
[18] | 王健云,周清木,秦平刚等.工业纯钛的缝隙腐蚀探讨[J].化工机械,2000,27(3):135 |
[19] | Satoh H,Shimogori K,Kamikubo F.The crevice corrosion resistance of some titanium materials[J].Platinum Met.Rev.,1987,31(3):115 |
[20] | Tsujikawa S,Kojima Y.Crevice corrosion-NaCl concentration map for grade-2 titanium at elevated temperature[J].Mater.Res.Soc.Symp.Proc,294,1993:311 |
[21] | Schutz R W.Understanding and preventing crevice corrosion of titanium alloys Ⅱ[J].Mater.Performance,1992,31(11):54 |
[22] | Yan L,No(e)l J J,Shoesmith D W,Hydrogen absorption into grade-2 titanium during crevice corrosion[J].Electrochim.Acta,2011,56:1810 |
[23] | Rajendran N,Nishimura T.Crevice corrosion monitoring of titanium and its alloys using microelectrodes[J].Mater.Corros.,2007,58(5):334 |
[24] | Vicentini B,Sinigaglia D,Taccani G.Crevice corrosion of titanium.Behaviour of galvanic cell between shielded and unshielded titanium in sulphuric acid[J].Corros.Sci.,1975,15(12):479 |
[25] | AbduIsalam M I,Pickering H W,The effect of crevice-opening dimension on the stability of crevice corrosion for nickel in sulfuric acid[J].J.Electrochem.Soc.,1998,145 (7):2276 |
[26] | AbduIsalam M I,Pickering H W.Effect of the applied potential on the potential and current distributions within crevices in pure nickel[J].Corros.Sci.,1999,41:351 |
[27] | Grauman J S.Beta-21S:A New High Strength,Corrosion Resistant Titanium Alloy[A].Proceedings of the international conference on titanium products and applications[C].Boulder:TDA,1990:290 |
[28] | Bergman D D,Grauman J S.The detection of crevice corrosion in titanium and its alloys through the use of potential monitoring[A].Titanium'92 Science and Technology[C].Warrendale:TMS,1992:2193 |
[29] | Brossia C S,Cragnolion G A.Effect of palladium on the corrosion behavior of titanium[J].Corros.Sci.,2004,46(7):1693 |
[30] | Kobayashi M,Araya Y,Fujiyama S,et al.Study on crevice corrosion of titanium[A].Proceedings of the 4th International Conference on Titanium[C].Warrendale:The Metallurgical Society of AIME,1980:2613 |
[31] | He X,Dunn D S,Csontos A A.Corrosion of similar and dissimilar metal crevices in the engineered barrier system of a potential nuclear waste repository[J].Electrochim.Acta,2007,52:7556 |
[32] | 褚武扬.氢损伤和滞后断裂[M].北京:冶金工业出版社,1988 |
[33] | Abdulsalam M I.Crevice corrosion of titanium in high temperature-concentrated chloride environments[J].J.Mater.Eng.Perform.,2007,16(6):736 |
[34] | Yan L,Ramamurthy S,No(e)l J J,et al.Hydrogen absorption into alpha titanium in acidic solutions[J].Electrochim.Acta,2006,52:1169 |
[35] | 伍怀龙,赵国庆,周筑颖等.氘在钛中的扩散行为[J].核技术,1996,19(6):326 |
[36] | Ogawa T,Yokoyama K,Asaoka K,et al.Hydrogen absorption behavior of beta titanium alloy in acid fluoride solutions[J].Biomaterials,2004,25(12):2419 |
[37] | Yokoyama K,Ogawa T,Asaoka K,et al.Hydrogen absorption of titanium in acidic fluoride solutions[J].Mater.Sci.Eng.,2004,A 384(1-2):19 |
[38] | Hirohata Y,Motojima D,Hino T,et al.Suppression of hydrogen absorption to V-4Cr-4Ti alloy by TiO2/TiC coating[J].J.Nucl.Mater.,2003,313-316:172 |
[39] | Nishimura R,Shirono J,Jonokuchi A.Hydrogen-induced cracking of pure titanium in sulphuric acid and hydrochloric acid solutions using constant load method[J].Corros.Sci.,2008,50:2691 |
[40] | Roy A K,Spragge M K,Fleming D L,et al.Cracking of titanium alloys under cathodic applied potential[J],Micron,2001,32(2):211 |
[41] | 卞敏,李英秋,刘钧等.高纯金属钛中微量氢的分析方法研究[J].稀有金属与硬质合金,2009,37(4):36 |
[42] | Blaauw M.Hydrogen precipitation in titanium observed with neutron incoherent scattering and prompt gamma neutron activation analysis[J].Nucl.Instrum.Methods Phys.Res.,Sect.,2003,505(1-2)A:20 |
[43] | Gibbons M R,Richards W J,Shields K.Optimization of neutron tomography for rapid hydrogen concentration inspection of metal castings[J].Nucl.Instrum.Methods Phys.Res.,Sect.,1999,424(1)A:53 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%