采用大功率EB-PVD工艺在NiO-YSZ多孔基体上制备了20 μm厚的YSZ电解质涂层材料.SEM分析表明制备态涂层表面由1 μm~10 μm的晶粒组成并含有少量微米级的孔隙,涂层材料的断面SEM表明涂层致密并和基体结合良好.EPMA分析显示初始蒸发阶段制备的涂层材料内Y,O元素分布均匀,Zr元素的分布存在一个梯度.XRD分析表明:涂层为典型的立方相结构并表现出择优取向特征.
参考文献
[1] | Schulz U;Fritscher K et al.[J].Surface and Coatings Technology,2000,133-134:40. |
[2] | Movchan BA.;Marinski GS. .Gradient protective coatings of different application produced by EB-PVD[J].Surface & Coatings Technology,1998(1/3):309-315. |
[3] | Lugscheider E.;Dopper G.;Barimani C. .Ceramic thermal barrier coatings deposited with the electron beam-physical vapour deposition technique[J].Surface & Coatings Technology,1998(1/3):1221-1227. |
[4] | Wolfe D E;Singh J et al.[J].Surface and Coatings Technology,2005,190:132. |
[5] | Jung Y C;Sasaki T et al.[J].Sci Tech Adv Mat,2003,4:571. |
[6] | Movchan M;Rudoy Y .[J].Materials & Design,1998,19:253. |
[7] | Guan C L;Zheng Z X et al.[J].Transactions of Nonferrous Metals Society of China,2005,15(03):61. |
[8] | Ma L;He X D;Li Y .[J].Transactions of Nonferrous Metals Society of China,2005,15(03):48. |
[9] | Woo S K;Shin T H.[A].Japan:the Electorc hemical Society of Japan,2004:2239. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%