Polycrystalline ZrO2-3 mol.%Y2O3 was brazed to Ti-6Al-4V by using a Ti47Zr28Cu14Ni11(at.%) amorphous ribbon at 1123–1273 K in a high vacuum. The influences of brazing temperature on the microstructure and shear strength of the joints were investigated. The interfacial microstructures can be described as ZrO2/TiO+TiO2+Cu2Ti4O+Ni2Ti4O/α-Ti+(Ti,Zr)2(Cu,Ni) eutectic/acicular Widmanst¨aten structure/Ti–6Al–4V alloy. With the increase in the brazing temperature, the thickness of the TiO+TiO2+Cu2Ti4O+Ni2Ti4O layer reduced, the content of the α-Ti+(Ti,Zr)2(Cu,Ni) eutectic phase decreased, while that of the coarse α-Ti phase gradually increased. The shear strength of the joints did not show a close relationship with the thickness of the TiO+TiO2+Cu2Ti4O+Ni2Ti4O layer. However, when the coarse (Ti,Zr)2(Cu,Ni) phase was non-uniformly distributed in the α-Ti phase, or when α-Ti solely situated at the center of the joint, forming a coarse block or even connecting into a continuous strip, the shear strength greatly decreased.

参考文献

[1] W.B.HANSON;K.I.IRONSIDE .ACTIVE METAL BRAZING OF ZIRCONIA[J].Acta materialia,2000(18/19):4673-4676.
[2] X.H. Wang,Y.C. Zhou.Layered Machinable and Electrically Conductive Ti2AlC and Ti3AlC2 Ceramics: a Review[J].材料科学技术学报(英文版),2010(05):385-416.
[3] O. Smorygo;J.S. Kim;M.D. Kim .Evolution of the interlayer microstructure and the fracture modes of the zirconia/Cu-Ag-Ti filler/Ti active brazing joints[J].Materials Letters,2007(2):613-616.
[4] A. V. Durov;B. D. Kostjuk;A. V. Shevchenko;Y. V. Naidich .Joining of zirconia to metal with Cu-Ga-Ti and Cu-Sn-Pb-Ti fillers[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2000(1/2):186-189.
[5] A. Rabinkin .Brazing with (NiCoCr)-B-Si amorphous brazing filler metals: alloys, processing, joint structure, properties, applications[J].Science and Technology of Welding and Joining,2004(3):181-199.
[6] M. Singh;R. Asthana;T.P. Shpargel .Brazing of ceramic-matrix composites to Ti and Hastealloy using Ni-base metallic glass interlayers[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2008(1/2):19-30.
[7] M. Singh;R. Asthana .Joining of zirconium diboride-based ultra high-temperature ceramic composites using metallic glass interlayers[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2007(0):153-162.
[8] Y.C. Kim;W.T. Kim;D.H. Kim .A development of Ti-based bulk metallic glass[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2004(0):127-135.
[9] Z.Y. Wu,R.K. Shiue,C.S. Chang.Transmission Electron Microscopy Study of the Infrared Brazed High-strength Titanium Alloy[J].材料科学技术学报(英文版),2010(04):311-316.