高级检索

采用传统的固相反应烧结工艺制备出了Ba1-3xBi2x(Ti0.9Sn0.1)O3(x=0,0.1%,0.2%,0.4%,0.6%,0.8%,1.0%,1.2%,1.4%)9种铁电陶瓷,利用XRD和介电温谱对陶瓷的物相结构与相变特性进行了研究.结果表明,产物为单相钙钛矿结构,Bi的A位轻量替代可以对陶瓷的介电性质和相变温度产生很大影响,随Bi元素在A位替代量的增加陶瓷从一般铁电体向驰豫铁电体转变,且弥散相变特征加重.

参考文献

[1] Ramplinga M J;Matherb G C et al.[J].Journal of the European Ceramic Society,2003,23:1911.
[2] Chen I W .[J].Journal of Physics and Chemistry of Solids,200,61:197.
[3] Chune Peng;Jing-Feng Li;Wen Gong .[J].Materials Letters,2005,59:1576.
[4] Yuana F;Pengc Z;Liua J M .[J].Materials Science and Engineering B,2005,117:265.
[5] Wenhui Ma;L. Eric Cross .Observation of the flexoelectric effect in relaxor Pb(Mg_(1/3)Nb_(2/3))O_(3) ceramics[J].Applied physics letters,2001(19):2920-2921.
[6] Granzow T Th Woike;W(o)hlecke M et al.[J].Physical Review Letters,2004,92(06):065701.
[7] Lu SG;Xu ZK;Chen H .Tunability and relaxor properties of ferroelectric barium stannate titanate ceramics[J].Applied physics letters,2004(22):5319-5321.
[8] Steinhausen R;Kouvatov A;Beige H et al.[J].Journal of the European Ceramic Society,2004,24:1677.
[9] Ludwig Geske;Volker Lorenz;Thomas Muller .Dielectric and electromechanical characterisation of fine-grain BaTi_(0.95)Sn_(0.05)O_3 ceramics sintered from glycolate-precursor powder[J].Journal of the European Ceramic Society,2005(12):2537-2542.
[10] Wenhui Ma;Eric Crossa L .[J].Applied Physics Letters,2002,18:3440.
[11] Bahri F;Khemakhem H;Simon A et al.[J].Solid State Sciences,2003,5:1235.
[12] Chen Ang;Zhi Yu;Zhi Jing .[J].Physical Review B,2000,61(02):957.
[13] Lines M E;Glass A M.Principles and Applications of Ferroelectrics and Related Materials[M].Oxford:Clarendon Press,1977:58.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%