以廉价的工业偏钛酸为原料,采用特殊的酸解工艺制得纳米级水合二氧化钛粉体,再利用高温管式炉对前驱体-TiO2·nH2O进行掺氮,制得纳米TiO2-xNx粉体,研究了不同掺氮气体和反应工艺对TiO2-xNx粉体吸光特性、形态结构的影响.结果表明水合TiO2粉体与氨气在600℃下反应5h,制得的粉体为锐钛矿型结构,粒径约为20nm,光吸收阀值由387nm红移至520nm左右.
参考文献
[1] | W F Zhang;M S Zhang;Z Yin.[J].Journal of Applied Physics B,2000:261. |
[2] | 岳林海,徐铸德.半导体的表面修饰与其光电化学应用[J].化学通报,1998(09):28-31. |
[3] | T Morkawa;R Asahi;T Ohwaki et al.[J].Journal of Applied Physics,2001,40:561-563. |
[4] | W Y Choi;A Termin;M R Hoffmann .[J].Journal of Physical Chemistry,1994,98:13669. |
[5] | A Giraudeau;F R F Fau;A J Bard .[J].Journal of the American Chemical Society,1980,102:5137. |
[6] | 施利毅,张怡,张潘琪,戴清,郭妍,袁春伟.纳米SnO2/TiO2复合颗粒形态结构表征[J].功能材料,2001(05):532-533,536. |
[7] | R Asahi;T Ohwaki;K Aoki .[J].科学(上海),2001,293:269-273. |
[8] | S Sato .[J].Chemical Physics Letters,1986,123:126. |
[9] | N C Saha;H G Tompkins .[J].Journal of Applied Physics,1992,72:3072. |
[10] | 张立德;牟其美.纳米材料学[M].沈阳:辽宁科学技术出版社,1994:95. |
[11] | 印永嘉.物理化学简明手册[M].北京:高等教育出版社,1988:370. |
[12] | F M Wiliam.Powder diffraction file.Alphabetical Index(Inorganic Material)[J].Swarthmore:JCPDS,1982 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%