含有磷、铜的CMnAl-TRIP钢板在820℃温度退火2min,然后分别在450℃和400℃贝氏体区等温不同的时间,研究了不同贝氏体等温温度对显微组织、力学性能和残余奥氏体稳定性的影响.结果表明CMnAl-TRIP钢具有优异的力学性能和延展性,450℃等温处理时钢板的各项力学性能优于400℃等温处理,而400℃等温处理试样中残余奥氏体的碳含量高,稳定性高,马氏体总体转变率低,导致低的应变硬化指数n值、均匀伸长率和总体伸长率.

参考文献

[1] Zackay V F;Parker E R;Fahr D D et al.The enhancement of ductility on high-strength steels[J].Trans of ASM,1967,60(02):252-259.
[2] Fischer FD.;Werner E.;Tanaka K.;Cailletaud G.;Antretter T.;Reisner G. .A new view on transformation induced plasticity (TRIP)[J].International Journal of Plasticity,2000(7-8):723-748.
[3] De Cooman BC .Structure-properties relationship in TRIP steels containing carbide-free bainite[J].Current opinion in solid state & materials science,2004(3/4):285-303.
[4] Zhao L;Moreno J;Kruijver S.Influence of intercritical annealing temperature on phase transformations in a high aluminium TRIP steel[A].Aachen:WMG,2001:141-145.
[5] Girault E;Jacques P;Harlet P .Metallographic methods for revealing the multiphase microstructure of TRIP-assisted steels[J].Materials Characterization,1998,40:111-118.
[6] Sugitomo K;Kobayashi M;Shirsawa H .Effects of second phase morphology on retained austenite morphology and tensile properties in a TRIP-aided dual-phase steel sheet[J].ISIJ International,1993,33:775-782.
[7] Krizan D;Antonissen J;Barbe L.Properties of austenite in micro-alloyed C-Mn-Al-Si-P TRIP steels[A].Chicago:David L Kanagy,2003:437-448.
[8] Itami A;Takahashi M;Usihioda K .Plastic stability of retained austenite in the cold-rolled 0.14%C-1.9%Si-1.7%Mn sheet steel[J].ISIJ International,1995,35:1121-1127.
[9] Sugimoto K;Usui N;Kobayashi M et al.Effects of volume fraction and stability of retained austenite on ductility of TRIP-aided dual-phase steels[J].ISIJ International,1992,32:1311-1318.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%