研究了非晶Sm5Fe74.3Nb1.5Si11.7B4.5C2.5Cu0.5合金经400℃,保温10min预退火后的晶化动力学.结果表明:该合金的晶化相为α-Fe固溶体和Sm2Fe17Cx金属间化合物,两相的晶化表观激活能分别为557kJ/mol和514kJ/mol.当晶化体积分数为60%时,α-Fe相的晶化激活能达极大值;Sm2Fe17Cx相晶化激活能则随其晶化体积分数的增加而逐渐减小.

参考文献

[1] Ralph Skomski;Coey J D .[J].Physical Review,1993,B48:15812.
[2] Chang W C;Chiou D Y;Wu S H .[J].Applied Physics Letters,1998,121:72.
[3] Ding J;McCormicks P G;Street R.[J].Journal of Magnetism and Magnetic Materials,1993(01):124.
[4] Schrefl T;Fidler J .[J].Journal of Applied Physics,1998,6262:83.
[5] Schrefl T;Fidler J;Onmü ller H K .[J].Physical Review,1994,B49:6100.
[6] 高文莉;隋智通;卢柯 .非晶态Pb-Cu-Si合金的晶化动力学研究[J].金属学报,1992,7:B304.
[7] Zhang J W;Zhang X Y;Xiao F R et al.[J].Materials Letters,1998,233:36.
[8] Zhang X Y;Zhang K Q;Liu J H et al.[J].Journal of Applied Physics,2001,1:89.
[9] 苗卫方;王景唐;李淑苓 .[J].金属学报,1990,26(04):B255-258.
[10] 卢柯;王景唐 .[J].金属学报,1990,26(05):B316-319.
[11] Kissinger H E .[J].Analytical Chemistry,1975,29:1702.
[12] 李余增.热分析[M].北京:清华大学出版社,1987:82.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%