欢迎登录材料期刊网

材料期刊网

高级检索

采用失重法、电化学极化曲线和电化学阻抗谱比较了0.5 mol/L HCl溶液中传统缓蚀剂苯并三唑(BTA)和辛酰谷氨酸、DL-苏氨酸、DL-丝氨酸等氨基酸类物质对铜的缓蚀作用.挂片试验和阻抗谱表明,10-3 mol/L的辛酰谷氨酸对铜的缓蚀作用最好,缓蚀率可以达到82.7%.从电化学极化曲线来看,这几种氨基酸类缓蚀剂均是阴极型缓蚀剂.在浓度10-5~10-3 mol/L范围内随着辛酸谷氨酸浓度升高缓蚀效果加强.

参考文献

[1] 张大全,高立新,周国定,陆柱.苯并三唑和8-羟基喹啉对铜的缓蚀协同作用[J].物理化学学报,2002(01):74-78.
[2] Boyd S;Ghaoui L El;Feron E.Linear Matrix lnequaities in System and Control Theory[M].Philadelphia:SIA M,1994:23-24.
[3] Moretti G;Guidi F;Grion G .Tryptamine as a green iron corrosion inhibitor in 0.5 mol/L deaerated sulphuric acid[J].Corrosion Science,2004,4(02):387-403.
[4] Saurbier K;Mendorf V;Schultze J W et al.Toluylanine as an inhibitor of atmospheric corrosion[J].Corrosion Science,1992,12(02):1351-1369.
[5] Moretti G;Guidi F;Grion G .Tryptamine as a green iron corrosion inhibitor in 0.5 mol/L deaerated sulphuric acid[J].Corrosion Science,2004,4(02):387-403.
[6] Kobler N;Ropital F;Estievenart C .Polyaspartates:Biodegradable alternates to polyacrylates or noteworthy multifunctional inhibitors[J].International Corrosion Denver,2002,4(11):45-78.