高速钢轧辊具有优异的耐磨性、抗粗糙性和抗热裂性,使用寿命是传统轧辊的3~5倍,采用高速钢轧辊能够大大降低换辊次数、辊耗和生产成本,同时,还可以提高轧件断面精度和表面质量.研究了两种不同工艺制造的高速钢热轧工作辊的微观组织特征和热疲劳性能,并讨论了制造工艺对组织和性能的影响.结果表明,从组织特征、使用性能和制造工艺复杂程度上来讲,CPC工艺制造的高速钢热轧工作辊表现出明显的优势.

参考文献

[1] Hwang K;Lee S;Lee H C .Effects of elements on microstructure and fracture properties of cast high speed steel rolls,part I:Microstructural analysis[J].Materials Science and Engineering A,1998,254(1-2):282-295.
[2] J.W.Park;H.C.Lee .Composition,microstructure,hardness,and wear properties of high-speed steel rolls[J].Metallurgical and materials transactions. A, physical metallurgy and materials science,1999(2):399-409.
[3] Rafael Colas;Jorge Ramirez;Ignacio Sandoval;Julio C. Morales;Luis A. Leduc .Damage in hot rolling work rolls[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,1999(1):56-60.
[4] Stevens P G;Kpivens;Harper P .Increasing Work-Roll Life by Improved Roll-Cooling Practice[J].Iron Steel Inst,1971,209(11):1-11,52.
[5] A. Molinari;A. Tremea;M. Pellizzari;A. Biggi;G. Corbo .High speed steels for hot rolls with improved impact and thermal fatigue resistance[J].Materials Science and Technology: MST: A publication of the Institute of Metals,2002(12):1574-1580.
[6] FU Hanguang;JIANG Zhiqiang;XING Jiahdong .The Effects of RE-Mg on Thermal Fatigue Resistance of Cast High Speed Steel (HSS) Rolls[J].Materials Science Forum,2005(Pt.1):217-220.
[7] 安运铮.热处理工艺学[M].北京:机械工业出版社,1982
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%