阐述了陶瓷内墙釉面砖吸湿膨胀的产生原因及降低吸湿膨胀的一般方法.针对某种产品吸湿膨胀率较大的问题,利用生产废料调整了生产配方.新试制产品在吸湿膨胀率方面符合国家标准要求,在其它主要性能方面也明显得到提高.