介绍了国外为适应阀门弹簧的高疲劳寿命对氧化物夹杂的苛刻要求,采用夹杂物形态控制理论使夹杂物无害化的生产技术,这种技术生产的超清洁阀门弹簧钢,细化和软化了氧化物夹杂,从而消除了氧化物夹杂对材料疲劳性能的危害,提高了阀门弹簧疲劳极限和寿命.
参考文献
[1] | 殷瑞钰.钢的质量现代进展(下篇).特殊钢[M].北京:冶金工业出版社,1995 |
[2] | T.Lund;R.Lyrberg .Valve Spring Wire Rod Manufacturing-[J].Wire Journal International,1984,17(08):64-71. |
[3] | Jun Kawahara;Koji Tanabe.Toshio Banno and Masashi Yoshida.Advance of Valve Spring Steel[J].Wire Journal International,1992(11):55-61. |
[4] | R.Kiessling;H.Nordberg.Inference of Inclusions on Mechanical Properties of Steel[A].,1970 |
[5] | R.Kiessling;H.Nordberg.Influence of Inclusions on Mechanical Properties of Steel.Critical Inclusion Size[A].Swedish Contribution IVA,1971 |
[6] | D.Brooksbank;K.W.Andrews.Thermal Expension of Some Inclusions Found in Steels and Relation to Tessellated Stresses[J].JISI,1968(06):595-599. |
[7] | D.Brooksbank.Thermal Expension of Calcium-Aluminate Inclusions and Relation to Tessellated Stresses[J].JISI,1970:495-499. |
[8] | D.Brooksbank;K.W.Andrews.Stress Field Rround Inclusions and Their Relation to Mechanical Properties[A].The Iron & Steel Istitute,1970:186-198. |
[9] | D.Brooksbank;K.W.Andrews.Stress Fields Around Inclusions and Their Relation to Mechanical Properities[J].JISI,1972(04):246-255. |
[10] | S.Rudnik .Discontinuities in Hot-Rolled Steel Caused by Non-Metallic Inclusions[J].JISI,1966,204(04):374-376. |
[11] | T.Malkiewicz;S.Rudnik.Deformation of Non-Metallic Inclusion During Rolling of Steel[J].The Journal of the Iron and Steel Institute,1963(01):33-38. |
[12] | G.Bernard;P.V.Riboud;G.Urbain.Oxide Inclusions Plasticity[J].Revue de Metallurgie-CIT,1981(05):421-433. |
[13] | S.Maeda;T.Soejima.Shape Control of Inclusion in Wire Rods for High Tensile Tire cord by Refining with Synthetic Slag[A].,1989:379-385. |
[14] | Hideaki;I.Ryo .Thermodynamics on Control of Inclusion Composition in Ultra Clean Steels[J].ISIJ International,1996,36(05):528-536. |
[15] | 曲英.炼钢学原理[M].北京:冶金工业出版社,1981 |
[16] | Hiroki Ohta;Hideaki Suito .Activities in CaO-SiO2-Al2O3 Slag and Deoxidation Equilibria of Si and Al[J].Metallurgical and Materials Transactions B:Process Metallurgy and Materials Processing Science,1996,27:943-953. |
[17] | Hideaki;I.Ryo .Thermodynamics on Control of Inclusion Composition in Ultra Chean Steels[J].ISIJ International,1996,36:298-310. |
[18] | G.K.Sigworth;J.F.Elliott .The Thermodynamics of Liquid Dilute Iron Alloys[J].Metal Science Journal,1974,18:298-310. |
[19] | S-W.Cho;H.Suito .Assessment of Calcium-Oxygen Equilibrium in Liquid Iron[J].ISIJ International,1994,34(03):265-269. |
[20] | 李正邦,薛正良,张家雯.弹簧钢夹杂物形态控制[J].钢铁,1999(04):20-23. |
[21] | Kiyosh Shiwaku;Jiro Koarai et al.Super Clean Steel for Valve Spring[J].R and D 神户制钢技报,1985,35(04):78-82. |
[22] | Toshiaki Hagiware.Super-clean Steel for Valve Spring Quality[J].Wire Journal International,1991(04):31. |
[23] | 齐藤诚 等.超清净ぽね钢[J].热处理,1987,27(01):23-30. |
[24] | Takehiko Ohshiro;Tatsuo Ikeda et al.Improvement of the Service Life of Valve Spring Wire[J].Stahl und Eisen,1989,109(21):35-39. |