以TiOSO4和TiOCl2为原料,合成出锐钛相和金红石相的相对含量分别约为85%和15%的纳米TiO2光降解催化剂. 在纳米TiO2表面担载质量分数为0.5%的银后,不但能较好地提高催化活性和使用寿命,而且表现出特有的絮凝作用,使催化剂易于分离,达到多次循环使用的目的. 对光催化降解活性黑模拟污水,以及蒽醌类染料、糖厂等实际污水发现,这种纳米TiO2具有活性高、寿命较长的特点,且能多次循环使用,降低了处理污水的成本.
参考文献
[1] | Frank S N. J Am Chem Soc[J],1977,99:4 667 |
[2] | Kamat P V. Chem Rev[J],1993,93:267 |
[3] | CUI Bin(崔斌),HAN Huan-Niu(韩欢牛),LI Shu-Ni(李淑妮), et al. Chin J Appl Chem(应用化学)[J],2001,18(12):958 |
[4] | NIU Xin-Shu(牛新书),XU Ya-Jie(许亚杰),SUN Rui-Xia(孙瑞霞), et al. Chin J Appl Chem(应用化学)[J],2002,19(9):898 |
[5] | Mills A,Davies R H,Worsley D. Chem Soc Rev[J],1993:417 |
[6] | Herrman J M. The Fifth International Conference on Photochemical Conversion and Storage of Solar Energy(Book of Abstracts)[C],Osaka,1984:15 |
[7] | Mcclune F W, Chief-Edr. Powder Diffraction File Alphabetical Index Inorganic Phases[M]. USA:JCPOS International Centre for Diffraction Data,1980 |
[8] | ZHANG Li-De(张立德),MU Ji-Mei(牟季美). Nano-material Science(纳米材料学)[M]. Shenyang(沈阳):Liaoning Science and Technology Press(辽宁科学技术出版社),1994 |
[9] | Dawson A,Kamat P V. J Phys Chem B[J],2001,105:960 |
[10] | ZHU Tun(朱屯),WANG Fu-Ming(王福明),WANG Xi-Dong(王习东), et al Chief-Edrs(主编). Overseas Recent Trends and Applications of Nano-material(国外纳米材料技术进展与应用)[M]. Beijing (北京):Chemical industry Press(化学工业出版社),2002 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%