采用铜模吸铸法制备出La62.0Al15.7(Cu0.5, Ni0.5)22.3大块非晶合金,并在室温和3.0~5.0 GPa压力条件下对该非晶合金进行了等温高压处理,研究了高压处理对该非晶结构弛豫和力学行为的影响.结果表明,高压处理对非晶合金的玻璃转变温度无明显影响,但使合金发生了明显的结构弛豫,其自由体积和第一晶化温度随压力的增加先增加后减小,最大值出现在4.0 GPa压力之下.纳米压痕和维氏硬度测试表明,其硬度值随压力变化规律与自由体积随压力变化规律一致.
参考文献
[1] | Akihisa Inoue .Amorphous, nanoquasicrystalline and nanocrystalline alloys in Al-based systems[J].Progress in materials science,1998(5):365-520. |
[2] | 杨志刚,王铁军,王高潮,杨刚.大块锆基非晶合金电化学耐腐蚀行为的试验研究[J].稀有金属,2004(01):25-28. |
[3] | Schuh C A;Nieh T G .A nanoindentation study of serrated flow in bulk metallic glasses[J].Acta Materialia,2003,51:87. |
[4] | Wang Weihua .Roles of minor additions in formation and properties of bulk metallic glasses[J].Progress in Materials Science,2007,52:540. |
[5] | Jin Haijun;Wen Ping;Lu Ke .Shear stress induced reduction of glass transition temperature in a bulk metallic glass[J].Acta Materials,2005,53:3013. |
[6] | Jiang Qingkui;Zhang Guoqing;Yang Liang;Wang Xiaodong Saksl K Franz H Wunderlich R Fecht H Jiang Jianzhong .La-based bulk metallic glasses with critical diameter up to 30 mm[J].Acta Materials,2007,55:4409. |
[7] | 蒲健,王敬丰,甘章华,易回阳,肖建中.块体Pd77.5Cu6Si16.5非晶合金的晶化动力学研究[J].稀有金属,2003(06):709-713. |
[8] | Yu Gengsheng;Lin Jianguo;Ma Mo;Wang Xiufeng,Wang Fenghua,Wen Cuier .Effect of relaxation on pressure sensitivity index in a Zr-based metallic glass[J].Materials Science and Engineering,2007,A460:58. |
[9] | Ming Xiang Pan;Jing Guo Wang;Yu Shu Yao;De Qian Zhao;Wei Hua Wang .Phase transition of Zr_(41)Ti_(14)Cu_(12.5)Ni_(10)Be_(22.5) bulk amorphous below glass transition temperature under high pressure[J].Applied physics letters,2001(5):601-603. |
[10] | Pan Mingxiang;Yao Yushu;Zhao Deqian;Zhuang Yanxin,Wang Weihua .Pressure-controlled nucleation and growth in Zr41Ti14Cu12.5Ni10Be22.5 bulk metallic glass close to and beyond glass transition temperature[J].Physics Letters A,2002,303:229. |
[11] | Yu P;Bai HY;Zhao JG;Jin CQ;Wang WH .Pressure effects on mechanical properties of bulk metallic glass[J].Applied physics letters,2007(5):51906-1-51906-3-0. |
[12] | Lee Y T;Welsch G .Young′s modulus and damping of Ti-6Al-4V alloy as a function of heat treatment and oxygen concentration[J].Materials Science and Engineering,1990,A128:77. |
[13] | Ruitenberg G;DeHey P;Sommer F;Sietsma J .Pressure-induced structural relaxation in amorphous Pd40Ni40P20: The formation volume for diffusion defects[J].Physical review letters,1997(24):4830-4833. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%