用AB腐蚀液对SI-GaAs晶片进行AB微缺陷显示 (AB微缺陷密度AB-EPD: 103~104 cm-2量级) ,用KOH腐蚀液显示位错(位错密度EPD: 104 cm-2量级),发现衬底上的位错对器件跨导没有明显的影响,而用AB腐蚀液显示的AB微缺陷对器件性能及均匀性有明确的影响: 低AB-EPD的片子跨导大; 高AB-EPD的片子跨导小.AB-EPD有一临界值,当AB-EPD高于此值时,跨导陡然下降.另外,还利用扫描光致发光光谱(PL mapping) 对衬底进行了测量,得出了与上述结果相符的结果.
参考文献
[1] | Miyazawa S;Ishida Y;Nanishi Y .Direct observation of dislocation effects on threshold voltage of a GaAs field-effect transistor[J].Applied Physics Letters,1983,43:853. |
[2] | Miyazawa S;Wada K .Mechanism for the threshold voltage shift of a GaAs field-effect transistor[J].Applied Physics Letters,1998,48:905. |
[3] | Suchet P;Duseaux M;Martin G M .Effects of dislocations on the threshold voltage of GaAs field-effect transistor[J].Journal of Applied Physics,1987,62:1097. |
[4] | 吴巨,何宏家,范缇文,王占国,张绵.半绝缘GaAs衬底中位错对MESFETs旁栅效应的影响[J].半导体学报,1997(07):558. |
[5] | Yamamoto H;Oda O et al.Microscopic defects in semi-insulating gaas and their effect on the FET device performance[J].Journal of the Electrochemical Society,1989,136(10):3098. |
[6] | 李光平,汝琼娜,李静,何秀坤,王寿寅,陈祖祥.SI-GaAs晶片的PL mapping表征技术[J].功能材料与器件学报,2000(04):365-368. |
[7] | 张泽兰,曾立波,齐芸馨.半绝缘砷化镓单晶中AB微缺陷的定量测量方法[J].分析测试技术与仪器,1999(01):45-47. |
[8] | 齐芸馨;孙毅之 .化合物半导体材料性能测试技术研究[R].总装备部预研管理中心, 信息产业部电子第四十六所,2000. |