在家电用彩涂板生产的卷取过程中会产生压斑缺陷,为了消除或减轻此种缺陷,本实验对其进行了研究,并用光泽仪对压斑缺陷进行了评价,在实验室模拟现场生产条件再现了家电用彩涂板压斑缺陷,研究了表面光泽以及温度对家电用彩涂板压斑缺陷的影响.结果表明,在其他条件相同的情况下,彩涂压斑缺陷的程度(试验前后正面光泽的变化)与彩涂板正反面光泽的差值以及环境温度有关.光泽差值越大,环境温度越高,产生压斑缺陷越明显.

参考文献

[1] LACOA JOSE IGNACIO IRIBARREN;VILLOTAB FRANCISCO CADENA;MESTRESC FRANCISCO LIESA .Corrosion protection of carbon steel with thermoplastic coatings and alkyd resins containing polyaniline as conductive polymer[J].Progress in Organic Coatings,2004,52(2005):151-160.
[2] 毛卫民.国产家电彩涂钢板分析[J].冶金丛刊,2000(05):11-12.
[3] 崔健.宝钢家电用钢的现状与发展[J].冶金丛刊,2000(05):16-19.
[4] HA EUN .The enhancement and evaluation method of adhesion force between coating and substrate[P].KR,GOIN1904,2006-02-03.
[5] B.A. Vermillion;J.T. Bousquet;R.E. Andrews;M. Thi;M.L. Hoppe;E.R. Castillo;A. Nikroo;D.T. Goodin;G.E. Besenbruch .DEVELOPMENT OF A NEW HORIZONTAL ROTARY GDP COATER ENABLING INCREASED PRODUCTION[J].Fusion science and technology: An international journal of the American Nuclear Society,2007(4):791-794.
[6] 刘昆.冷轧薄板带卷取机传动控制[J].湖南冶金,2004(02):22-26.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%