天然石墨(NG)分别掺入碳纳米管(CNT)和纳米炭粉(CNP),得到两种纳米炭与石墨碳的混合材料.通过比较NG、CNT、CNP及其混合材料分别作为锂离子电池负极时的电化学性能,发现碳纳米管的首次不可逆容量损失很大,它的混合材料也不适合作锂离子电池的负极材料; 纳米炭粉与石墨有很好的协同效应,该混合材料具有良好的电化学性能,相同条件下与天然石墨相比,其充放电比容量分别提高9.8%和9.4%.
参考文献
[1] | Tsutomu O, Yasunobu I, Keijiro S. J. Electrochem. Soc., 1993, 140: 2490-2496. |
[2] | Xiang H Q, Fang S B, Jiang Y Y. J. Power Sources, 2001, 94: 85-91. |
[3] | Hossain S, Kim Y K, Saleh Y, et al. J. Power Sources, 2003, 114: 264-276. |
[4] | Li H, Huang X J, Chen L Q. J. Power Sources, 1999, 81/82: 335-339. |
[5] | Guo K, Pan Q M, Fang S B. J. Power Sources, 2002, 111: 350-356. |
[6] | Wu Y P, Jiang C Y, Wan C R, et al. Electrochemistry Communications, 2000, 2: 272-275. |
[7] | Sumura T, Katanosaka A, Souma I, et al. Solid State Ionics, 2000, 135: 209-212. |
[8] | Gupta V, Nakajima T, Ohzawa Y, et al. J. Fuorine Chemistry, 2001, 112: 233-240. |
[9] | Wu Y P, Jiang C Y, Wan C R, et al. Electrochemistry Communications, 2000, 2: 626-629. |
[10] | Read J, Foster D, Wolfenstine J, et al. J. Power Sources, 2001, 96: 277-281. |
[11] | Wilson A M, Dahn J R. J. Electrochem. Soc., 1995, 142: 326-332. |
[12] | Che G L, Lakshmi B B, Fisher E R, et al. Nature, 1998, 393: 346-349. |
[13] | Che G L, Lakshmi B B, Martin C R, et al. Langmuir, 1999, 15: 750-758. |
[14] | Nalimova V A, Sklovsky D E, Bondarenk G N, et al. Synthetic Metals, 1997, 88: 89-93. |
[15] | Frackowiak E, Gautier S, Gaucher H, et al. Carbon, 1999, 37: 61-69. |
[16] | Wu G T, Wang C S, Zhang X B. J. Electrochem. Soc., 1999, 146: 1696-1701. |
[17] | Fong R, Sacken U, Dahn J R. J. Electrochem. Soc., 1990, 137: 2009-2013. |