研究了氧含量对Ni47Ti44Nb9合金显微组织和相变行为的影响.结果表明,当氧含量超过固溶度后,氧存在于(Ti,Nb)4Ni2O氧化物中.随着氧含量的增加相变温度降低,应力诱发马氏体相变的临界应力提高,相变热滞变宽.氧含量(质量分数)在0.04%-0.07%范围内,Ni47Ti44Nb9合金具有最大的形状记忆应变和延伸率.
参考文献
[1] | Melton K N, Simpson J, Duerig T W. Proc Int Conf on Martensitic Transformation, 1986:1053 |
[2] | Melton K N, Proft J L, Duerig T W. Proc MRS Int Meeting on Advanced Materials, 1988; 9:165 |
[3] | Zhang C S, Zhao L C, Duerig T W, Wayman C M. Scr Metall Mater, 1990; 24:1807 |
[4] | Piao M, Miyazaki S, Otsuka K, Nishida N. Mater Trans JIM, 1992; 33:337 |
[5] | Jackson C M, Wagner H J, Wasilewski R J. NASA, 1972:15 |
[6] | Xu D S, Song Y, Li D, Hu Z Q. Philos Mag, 1997; A75:1185 |
[7] | Otsuka K, Wayman C M. Shape Memory Materials. 1998:71 |
[8] | Proft J L, Duerig T W. Engineering Aspects of Shape Memory Alloys. 1990:21 |
[9] | Jin W, Dong S Z, Jin Y B, Cao M Z. Proc China-Japan Bilateral Symposium on SMAs, 1998:65 |
[10] | 杨大智,张连生,王风庭.形状记忆合金.1988:4 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%