采用传统固相反应法制备了Ba(Ti0.96Sn0.04)O3无铅压电陶瓷,对其压电性能、介电性能、铁电性能和微观结构等进行了研究.研究发现,原料以及制备工艺对Ba(Ti0.96Sn0.04)O3陶瓷的压电性质具有较大的影响.与BaTiO3陶瓷相比,Ba(Ti0.96Sn0.04)O3陶瓷的正交-四方相变温度To-T得到了一定的提高,并且To-T附近的热滞只有1.8℃.陶瓷的微观形貌呈现出较为复杂的畴结构,主要以90°平行带状畴为主,偶尔有少量不同构型的180°畴.电滞回线呈现为理想的近似矩形饱和形状的曲线,剩余极化强度Pr为18.9 μC/cm2,矫顽场Ec为2.5 kV/cm.此外,非180°畴的翻转是引起陶瓷逆压电常数d33*的主要因素,其值可达550 pm/V.
参考文献
[1] | Jurgen Rodel;Wook Jo;Klaus T. P. Seifert.Perspective on the Development of Lead-free Piezoceramics[J].Journal of the American Ceramic Society,20096(6):1153-1177. |
[2] | P. Zheng;J.L. Zhang;Y.Q. Tan.Grain-size effects on dielectric and piezoelectric properties of poled BaTiO_3 ceramics[J].Acta materialia,201213/14(13/14):5022-5030. |
[3] | J. L. Zhang;P. F. Ji;Y. Q. Wu;X. Zhao;Y. Q. Tan;C. L. Wang.Strong piezoelectricity exhibited by large-grained BaTiO_3 ceramics[J].Applied physics letters,201422(22):222909-1-222909-4. |
[4] | Tan, Yongqiang;Zhang, Jialiang;Wang, Chunlei;Viola, Giuseppe;Yan, Haixue.Enhancement of electric field-induced strain in BaTiO3 ceramics through grain size optimization[J].Physica status solidi, A. Applications and materials science ePSS,20152(2):433-438. |