欢迎登录材料期刊网

材料期刊网

高级检索

针对河北某金矿矿石自然金粒度大小不等、嵌存状态复杂的特点,采用尼尔森重选-浮选工艺流程回收金取得了较为理想的指标。尼尔森选矿机处理一段磨矿产品回收中粗粒金,获得品位291 g/t、回收率26.71%的重选金精矿。尼尔森中矿并入尾矿一起再磨至-0.074 mm占85%,以丁基黄药和M-钠盐组合捕收剂强化金的浮选,获得品位122.7 g/t、回收率62.35%的浮选金精矿,金总回收率达到89.06%。相比单一浮选流程,金回收率提高3.57%。

Considering the characteristics of different sized native gold and complex embedding conditions of one gold ore,Nelson gravity-flotation process is used to recover gold and achieves satisfactory results .Nelson processing machinery treats the first-stage grinding products and recovers medium and large sized gold particles ,obtaining gravity separation gold concentrates with grade of 291 g/t and recovery rate of 26.71 %.Nelson middlings are mixed with tailings and together grinded to 85 % -0.074 mm.Combined collector of Butyl Xanthate and M-sodium salt is used to enhance gold flotation,obtaining flotation gold concentrates with grade of 122.7 g/t and recovery rate of 62.35%. Overall gold recovery rate reaches 89.06%and compared to single flotation process ,gold recovery rate is increased by 3 .57 %.

参考文献

[1] 胡熙庚.有色金属硫化矿选矿[M].北京:冶金工业出版社,1987
[2] 马科友,王洪凯,吕久吉.提高金银浮选回收率的试验研究[J].有色矿冶,2010(02):16-18.
[3] 董兵,任华杰.小秦岭某矿石金、铜回收试验研究[J].黄金,2009(06):46-48.
[4] 张金钟,姜良友,吴振祥,罗中兴.尼尔森选矿机及其应用[J].有色矿山,2003(03):28-31,37.
[5] 石凤野,王彦慧.尼尔森重选设备在金滩矿业公司的应用[J].黄金,2013(03):58-60.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%